    Well a buddy of mine bought this up pipe for his 09' WRX and it came with a flange for a 44mm tial wastegate. He bought a wyntomn wastegate and of course the flanges were different. So we used a hack saw to saw off the old flange at the welds and I decided I would weld on the new flange for him.

    The machine was running at about 70 amps with about 10-20 pulses a second. Here are some pictures during the process.

    Here is a picture of the up pipe with the old flange cut off and the new flange to be welded on.






    Here are a couple pictures of the final product.





    Brandon Raineri
    The Pennsylvania State University
    Studying Industrial Engineering

    Everlast PowerPro 205
    Everlast I-Mig 200
    SpeedGlas 9100x
    Milwaukee 14" Dry Cut Saw
    Craftsman 6"x48" Belt Sander with 9" Disc Sander

  2. #2

    Default

    Thats what I like about having a welder. You can make anything work..
    Aloha from Hawaii
    PowerTig 250EX
    A wallet that still has something in it from the great value I got!

  3. #3

    Default

    That looks great, what filler did you use. I want to start playing with all that
    Journeyman welder
    250EX
    Power plasma 60
    horizontal band saw
    Miller digital elite 'wicked' lid

  4. #4

    Default

    Thats nice looking. Any idea what stainless alloy is?
    Its nice being able to making things work at your hearts desire, isn't it.
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  5. #5

    Default

    yeah its very nice to be able to just do whatever and make it work. I believe the up pipe is 16ga T-304 and the filler used was 1/16 308L
    Brandon Raineri
    The Pennsylvania State University
    Studying Industrial Engineering

    Everlast PowerPro 205
    Everlast I-Mig 200
    SpeedGlas 9100x
    Milwaukee 14" Dry Cut Saw
    Craftsman 6"x48" Belt Sander with 9" Disc Sander

Similar Threads

  1. Project #3 Dyethor, Pipe flange tool
    By dyethor in forum Other Custom Fabrications
    Replies: 6
    Last Post: 02-21-2012, 02:44 PM
  2. Replies: 4
    Last Post: 07-18-2011, 03:10 AM
  3. Wastegate repair (aluminum TIG build-up)
    By jakeru in forum Welding Repairs
    Replies: 4
    Last Post: 03-07-2011, 06:24 PM
  4. Replies: 0
    Last Post: 03-05-2011, 01:43 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •