How to check weld penetration. Acids,Bluing,Rusting, What works? My research revealed
If this is your first visit, be sure to check out the
FAQ
by clicking the link above. You will have to
register
before you can post: click the register link above to proceed. To start viewing messages, select the forum that you want to visit from the selection below.
Share
Tweet
Results 1 to 19 of 19
Thread:
How to check weld penetration. Acids,Bluing,Rusting, What works? My research revealed
Thread Tools
Show Printable Version
Display
Switch to Linear Mode
Switch to Hybrid Mode
Threaded Mode
Threaded View
I_Love_Plasma
How to check weld...
12-28-2011,
10:27 PM
sportbike
You can try Muriatic acid...
12-28-2011,
10:55 PM
I_Love_Plasma
Thanks for the suggestions. I...
12-28-2011,
11:02 PM
sportbike
Hmm...didn't see that you...
12-28-2011,
11:15 PM
I_Love_Plasma
I took that same piece,...
12-29-2011,
01:16 PM
donor76
When I worked at factory...
12-29-2011,
02:55 PM
I_Love_Plasma
I'm sorry, I am having...
12-29-2011,
04:13 PM
Joe from NY
Remember donor76 is in...
12-30-2011,
09:52 PM
Tritium
A solution of nitric acid and...
12-31-2011,
04:45 AM
I_Love_Plasma
Some new pictures of etching....
01-31-2012,
05:54 PM
redbeard
I believe he did mention...
12-31-2011,
05:37 AM
I_Love_Plasma
Thank you for the link...
01-02-2012,
05:55 PM
donor76
Yes my friends, I communicate...
12-31-2011,
06:18 AM
Joe from NY
Брат, мы рады видеть вас...
12-31-2011,
03:49 PM
donor76
Guys happy New Year!!! ура!!!
12-31-2011,
05:11 PM
Joe from NY
Donor- was my Russian...
12-31-2011,
08:13 PM
donor76
I rejoice(on Russian)
12-31-2011,
08:49 PM
More replies below current depth...
Previous Post
Next Post
12-31-2011,
08:13 PM
#16
Joe from NY
View Profile
View Forum Posts
Private Message
View Blog Entries
View Articles
Member
Join Date
Dec 2011
Location
Long Island, New York
Posts
235
Donor- was my Russian translation correct, what did it say?
Reply With Quote
Quick Navigation
Metal Art
Top
Site Areas
Settings
Private Messages
Subscriptions
Who's Online
Search Forums
Forums Home
Forums
Everlast Community
Everlast Announcements, Contests and Promotions
Forum related Questions
Introduce Yourself
Customer Testimonials
Pre-sales, Sales and Shipping questions
Everlast Plasma Cutters
Everlast Plasma Cutters (PAC)
Everlast Welders
TIG Welding (GTAW/GTAW-P)
Stick Welding (SMAW)
MIG Welding (GMAW/GMAW-P/FCAW)
Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
Technical Bulletins and Tips
Welding Talk
General Welder Questions
General Welding Questions
Welding Projects and Pictures
Metal Art
Hobyist Projects
Welding Repairs
On Road Fabrication
Off Road Fabrication
Other Custom Fabrications
Heavy Equipment and Commercial Projects
Automated welding system (CNC), Submerged ARC, etc.
Welding articles from Professionals (knowledge database)
Off Topic
General Chat Lounge
Personal Projects (no welder required)
Truck, Car and Bike builds
Tips & Tricks, Custom Tools, Safety, Ideas and Reviews.
Buy, Sale or Trade
«
Previous Thread
|
Next Thread
»
Similar Threads
3G 6010 full penetration welds, I can't do, and I'm running out of plate!
By GaveUpOnTV in forum Stick Welding (SMAW)
Replies:
12
Last Post:
06-21-2023,
06:37 AM
Mystery Welder Revealed: 2012 DIGITAL POWERTIG 210EXT TIG/STICK welder
By performance in forum Everlast Announcements, Contests and Promotions
Replies:
46
Last Post:
07-28-2012,
02:19 AM
Penetration of weld and weld build up?
By CGCINC in forum General Welding Questions
Replies:
4
Last Post:
07-03-2012,
07:06 AM
Posting Permissions
You
may not
post new threads
You
may not
post replies
You
may not
post attachments
You
may not
edit your posts
BB code
is
On
Smilies
are
On
[IMG]
code is
On
[VIDEO]
code is
On
HTML code is
Off
Forum Rules