Machine showed up tuesday evening and i been digging around here for a few weeks making sure i got all the other pieces in place to use it as soon as it arrived.
Got a tracking number shortly after placing my order and had no issues with UPS on this welder as well.
Guy at lowes gave me incorrect breaker for the panel box and i thought the welder was DOA.
Quick phone call in and Ray walked me through the screw up and i got it up and going. I dont have much of an issue with steel but i still got a long way to go until my stuff is decent.
Anyway had a little trouble with the plasma(or so i thought) and again i had no problem getting in touch with customer support and after a process of elemination I found out that i was most likely not moving the tip fast enough. After i figured it out it was nice to use. Overall I am extremely pleased with the unit.

Here are a few pics of my setup and some of my progress. I know its not pretty but i think i have done well for just 1 day of practice and getting the settings nailed down.








1 Thing i did note, Was start/end amps, up slope and down slope work with the foot pedal plugged in and it kind of threw me for a loop as i only expected these to work on the 4t switch mode for the torch! But now that i know its works fine.
Tig welder seems to have plenty of power as well as the plasma. All features seem to work. Pedal,trigger, up slope,down slope, start/end amps, pulser works as well. Very nice machine for the money.
I will try and post some of my projects as i will be doing a lot of cars this year and a few turbo ones that require some aluminum fab work.
As soon as i get this down pat i will work on some chrome moly as i intend to do cages with this thing.

Any reccomendations on a nicer torch for the cages? Mostly smaller i guess.


Thanks
Everlast.