    Need a little help , most everything i weld is steel. Want to weld a intake manifold that has a crack approx 1/2 thick aluminum, i have already v'd the crack, any one give me a general start settings on my 200dx ?? I'd appreciate any info.

  2. #2

    Default

    You are really going to be above teh capacity of the 200dx to weld it "right. that said, you may still be able to weld it.

    You will definitely be at full power, and pretty much adjust everything it's got to focus the arc for penetration. If you can get a helium mix for your gas it woudl be better, but probably not practical for one weld.

    To get it to work well, you are going to have to preheat the part. If you have a torch that may work, but a better option would be to put it in an oven to get the whole part up to temp. I'd go to about 400-450 on that since you don't have to worry about any over-aging for a cast manifold.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  3. #3
    Join Date
    Feb 2011
    Location
    Fridley, Minnesota
    Posts
    376

    Default I agree with Sportbike, but here's another option

    I agree with Sportbike, as far as trying to get the job done in TIG mode with a 200dx, but, if you're unable to get that to work, the other option is ESAB's "Allstate Smoothcote 34" Electrodes. They are an aluminum alloy electrode meant to run on DCEP, and the 200dx, in stick mode, should prove to be the PERFECT machine to run them with. Below is a quote from their website describing them. They are available in 3/32" and 1/8"

    "A premium DC reverse, all-position aluminum electrode with an extruded coating. For use on aluminum sheets, plates and castings of 1/8" thickness or heavier. Deposits are dense and smooth, and provide good color match to base metal. Also for build-up, cladding and reinforcing."

    There's actually a guy from Finland or some other eastern-bloc that has you-tube videos posted using these (or similar) electrodes to perform some aluminum welding in DC-TIG mode! Although far from ideal, it just goes to show what a person is capable of when it comes time to improvise.

    I must include a disclaimer that I have NO personal experience with either the electrodes, or the 200dx, so, this is just an idea that, if all else fails, I put out there for you to investigate further, either way, wish you the best of luck!
    "It's not magic it's experimental, kind of like washing your hands after pooping used to be." -House

    Everlast PowerTig 250EX-arrived 1-26-2012
    Everlast PowerCool W300-arrived 1-26-2012
    Everlast PowerTig 185 Micro-arrived 1-26-2012
    Everlast PowerPlasma 70-arrived 1-26-2012
    ESAB MigMaster 250-borrowed
    HyperTherm 151 AKA "The Light Sabre"
    Linde UCC-305-964 lb. of old time water cooled TIG love-SOLD-Bad MOJO
    Purox OXY/ACETYLENE

  4. #4
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Interesting thread- Bobkat, please let us know how it goes.

    Sportbike's post mentions preheating, and I wondered if the stick electrode method required any preheating. Based on Hooda's post I searched for "ESAB Allstate Smoothcote 34", saw a link to the ESAB site, and found that ESAB graciously posts a procedure! Turns out there is a preheat and postheat / cooldown.

    Procedure
    Clean weld area thoroughly. Any base metal heavier than 1/8"( 3.2mm) should be beveled at a 75 degree angle. No preheating is necessary on thin material but on heavy sections preheating to 400°F (204°C) is recommended to flatten the weld bead and reduce the amount of amperage required. Stringer beads are generally used since some undercutting will be encountered with weave beads. A short arc should be maintained with the electrode tilted slightly in the direction of travel. Allow to cool slowly. Remove slag before quenching. Additional cleaning and slag removal may be done with a wire brush and a solution of 5% nitric or 10% sulfuric acid in hot water. Rinse with clean, hot water.
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  5. #5
    Join Date
    Dec 2011
    Location
    RUSSIA.Sankt Peterburg
    Posts
    218

    Default

    Ruslan
    EVERLAST Power Tig 255 EXT
    EVERLAST PP256
    PC300
    EWM Pico 162
    MERKLE mobimig 180K
    SELCO Genesis 352 pme

  6. #6

    Default

    Quote Originally Posted by donor76 View Post
    that video reminds me of the old guy at all the car shows and swap meets always welding up holes he had punched in soda cans with special rods and a propane torch.

  7. #7

    Default

    Quote Originally Posted by hooda View Post
    I agree with Sportbike, as far as trying to get the job done in TIG mode with a 200dx, but, if you're unable to get that to work, the other option is ESAB's "Allstate Smoothcote 34" Electrodes. They are an aluminum alloy electrode meant to run on DCEP, and the 200dx, in stick mode, should prove to be the PERFECT machine to run them with. Below is a quote from their website describing them. They are available in 3/32" and 1/8"

    "A premium DC reverse, all-position aluminum electrode with an extruded coating. For use on aluminum sheets, plates and castings of 1/8" thickness or heavier. Deposits are dense and smooth, and provide good color match to base metal. Also for build-up, cladding and reinforcing."

    There's actually a guy from Finland or some other eastern-bloc that has you-tube videos posted using these (or similar) electrodes to perform some aluminum welding in DC-TIG mode! Although far from ideal, it just goes to show what a person is capable of when it comes time to improvise.

    I must include a disclaimer that I have NO personal experience with either the electrodes, or the 200dx, so, this is just an idea that, if all else fails, I put out there for you to investigate further, either way, wish you the best of luck!
    Thanks that looks interesting, i have at my shop a miller 250 dial arc hf, i have the 200dx at my house, might add the crack is less than 1/4 deep

  8. #8

    Default

    that looks way to easy, wonder if it really works?

  9. Default

    Quote Originally Posted by bobkat View Post
    that looks way to easy, wonder if it really works?
    Bobkat,

    Hope you let us know if you give it a shot.
    With pics.

    Cheers,
    rivets

  10. #10
    Join Date
    Feb 2011
    Location
    Fridley, Minnesota
    Posts
    376

    Default I'm SKEPTICAL on the HTS-2000 BEWARE!!

    Quote Originally Posted by donor76 View Post
    Donor76'S suggestion of the HTS-2000 rods may be well intended, but it you were to try it, please experiment with another, non-critical piece before you go after your important piece. Someone else mentioned that it reminded him of the guy selling a similar product at swap-meets. I've bought it, and it does a great job brazing 2 pop cans together, but for everything else I tried it on, it was WORTHLESS! What I found out is that it's not a "variant", which would suggest that it's an aluminum rod, but rather a solder or brazing alloy containing a large percentage of zinc and other metals in their "secret recipe" that's SUPPOSED to stick to aluminum. My experience was "not so much". Another perspective is that, if it were all it claims to be, a major manufacturer would have picked up on it by now. Good Luck!
    "It's not magic it's experimental, kind of like washing your hands after pooping used to be." -House

    Everlast PowerTig 250EX-arrived 1-26-2012
    Everlast PowerCool W300-arrived 1-26-2012
    Everlast PowerTig 185 Micro-arrived 1-26-2012
    Everlast PowerPlasma 70-arrived 1-26-2012
    ESAB MigMaster 250-borrowed
    HyperTherm 151 AKA "The Light Sabre"
    Linde UCC-305-964 lb. of old time water cooled TIG love-SOLD-Bad MOJO
    Purox OXY/ACETYLENE

  11. #11

    Default hts rods

    Quote Originally Posted by hooda View Post
    Donor76'S suggestion of the HTS-2000 rods may be well intended, but it you were to try it, please experiment with another, non-critical piece before you go after your important piece. Someone else mentioned that it reminded him of the guy selling a similar product at swap-meets. I've bought it, and it does a great job brazing 2 pop cans together, but for everything else I tried it on, it was WORTHLESS! What I found out is that it's not a "variant", which would suggest that it's an aluminum rod, but rather a solder or brazing alloy containing a large percentage of zinc and other metals in their "secret recipe" that's SUPPOSED to stick to aluminum. My experience was "not so much". Another perspective is that, if it were all it claims to be, a major manufacturer would have picked up on it by now. Good Luck!
    I am thinking the esab smoothcote rods are looking pretty good, going to see if my local has them.

Similar Threads

  1. MIG welder settings
    By L98fiero in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 1
    Last Post: 01-20-2018, 04:48 AM
  2. Mystery Welder Revealed: 2012 DIGITAL POWERTIG 210EXT TIG/STICK welder
    By performance in forum Everlast Announcements, Contests and Promotions
    Replies: 46
    Last Post: 07-28-2012, 03:19 AM
  3. Everlast Tig Welder settings
    By revkev6 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 03-04-2011, 03:23 PM
  4. ac tig settings
    By iil in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 12-24-2010, 01:46 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •