Good thing to practice on.
By the way the correct filler for 4130 cm tubing is NOT 4130 filler. 4130 filler should only be used if the parts will be heat treated. Most use an er70 or er80 filler with 4130 tubing.
Good thing to practice on.
By the way the correct filler for 4130 cm tubing is NOT 4130 filler. 4130 filler should only be used if the parts will be heat treated. Most use an er70 or er80 filler with 4130 tubing.