I have made up a few of these quick change drain pans while finishing up my TIG Welding classes. They are 12" long, 10" wide, and 3" deep. It has a shelf with drain holes to set gears on while changing. Perfect for those gear changes done at the track. Its made from 3003 aluminum. 2 of them have a couple blotchy welds, but its purely cosmetic and functionality remains the same. Im considering making more but well see how it goes.

All done with my 200dx

I have 4 of these now.

$35.00 plus $7.00 shipping per pan OBO.

Thanks for looking, JB

Im in NorthWestern NC