    do you have plans on making a tungsten grinder ??

  2. #2

    Default

    Gene,

    We have been searching for one that won't take your hand off in the grinding process.

    We started looking quite a while ago. This is an item that would be "drop in" for our line. We would simply source a ready to go unit from an existing manufacturer and not go into providing specs, and changes, because right now demand is fairly low for that product and extended product development would not be worth it. The search is on, in other words, but we have rejected all designs so far...for one reason or the other.

  3. #3
    Join Date
    Aug 2009
    Location
    North of Dallas Tx
    Posts
    39

    Default

    i bought chem-sharp and it made a needle point in about 20 seconds...no grinding.

    http://store.weldersource.com/chemsharp.html
    Gnothi Seauton 515 rwhp/527 Lbs.@21psi....nuff said.
    http://i156.photobucket.com/albums/t...ax_Modsico.jpg
    2JZ-HX40 Turbo swap Conquest. SDS-6E ECU, turbo pistons & HG, ACL race bearings, Arps, Custom FFIM for 1000cc injectors ..E-85 daily driven.

    http://i156.photobucket.com/albums/t...t/DSC01364.jpg

    2009 FZ1N Retro
    PowerTig 200LX to make things possible.

  4. #4

    Default

    Dax, it works and does a good job,your right.

  5. #5
    Join Date
    Mar 2011
    Location
    Orlando, Florida
    Posts
    38

    Default

    How fast does the Chem Sharp works and does it leave a residue on the Tungsten that has to be cleaned or you can go right on welding?
    Peter

  6. #6

    Default

    Does the Chem sharp work well on new tungsten or just for resharpening already ground rods? It seems to be the way to go for me I will most likely do little tig welding and most likely ruin a lot of tips during my learning process. Any thoughts?
    Ray
    Last edited by Ram48; 03-13-2011 at 01:02 AM. Reason: sp.

Similar Threads

  1. Replies: 0
    Last Post: 02-08-2016, 05:11 PM
  2. Tungsten grinder question
    By Ram48 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 09-06-2011, 05:53 PM
  3. Tungsten Grinder
    By NRM in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 1
    Last Post: 07-22-2011, 01:03 AM
  4. Pics of my $19.98 Tungsten grinder setup
    By hooda in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 04-28-2011, 10:45 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •