Yes you read that correct, a coffin gas tank. My buddy has a small 50cc chopper and he wants a bigger motor in it. So we stripped it all down. I made a deal with him so now im makin his tank. Dont ask me why he wants a coffin, all im doing is building it. Im using 1/16" sheet metal. Its about 1' long, 7" at the widest and 4" deep. I build the rough box tonight while i was waiting for the vht to dry on my taillights. Tommorrow i will make a tunnel for the bottom so it can slide down onto the frame. Heres what i did tonight...
![]()