Post your favorite settings on a 200DX for aluminum?
Can anyone advise what settings to start with on my 200DX to practice on a piece of 1/8" aluminum? I grabbed a piece of flat stock to practice on, and i blew holes in it, and melted my torch nozzle, and the end of my tungsten looks like a golf ball. I have 3/32 Red tungsten, with a WP9 torch. i will start with the torch switch before trying out the pedal. I am looking to find out what settings the brothers recommend for this machine to not blow up the torch, and make a big mess out of the aluminum. I destroyed three nozzles already.
thanks
Last edited by Joe from NY; 01-21-2012 at 08:47 PM.
Some of the crap I use to keep busy:
Everlast 200DX
Millermatic 211 Mig
Hypertherm Powermax 30 plasma cutter
Lincoln Weld-Pak 100
Century Stick welder
Oxy set-up with Henrob 2000 torch
Logan 200 lathe (60 years old)
Jet band saw
About 6 Harbor Freight grinders with different discs/wheels/brushes