    Default Tig Start Question

    I am new to tig, and do not even have an Everlast yet...but looking. I have a Chiri UNT 3-in-1 unit. I would have asked on the WW forum, but expected I would get flamed for having a chinese unit. Everything works fine, except I have a question about initial startup.

    I am using a WP-17 torch (no pedal), 1/16" 2% lanthanated sharp, Argon at 11cfh. Today welding 1/8" angle, with 1/16" 70S-6 filler, 65amps. This action has happened on other thicknesses of metal, and amp settings also.

    When I first press the lever to initiate a weld, at once, the arc jumps and there is a POP. Like a small balloon being punctured. Then all settles down, and seems ok. Is this normal? It does not happen every time, random, as far as I can tell.

    Not sure if it is argon, or only when I have too much distance from the work (long arc initially). The flowmeter could be incorrect, but I can get a good puddle and the weld looks fairly decent for a learner. So I think I have correct flow.

    Any ideas I could check out further? I expect is probably operator induced if it is a problem.

  2. #2

    Default

    Try pressing the trigger a few times off of the part to get the argon to purge out of the hoses, then immediately go to your workpiece and try an arc start.

    This may not be the problem, but certainly worth a try.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  3. #3

    Default

    You are welding in DC mode, correct ?
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  4. #4

    Default

    Is your Tig Torch hooked up to the negative terminal? Half the battle of Tig welding is learning how to use/set the machine!
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  5. #5

    Default

    zoama, yes, DC...only have DC.
    Sean...yes, all is hooked up properly...tig connects to air port and the 7pin control, work clamp to positive.
    Sportbike, I will try the purge action today.

    thank you

  6. #6

    Default

    Check your argon hoses, too... you may have a leak in your hose line.
    open the argon bottle, and hit the pedal to purge the line. After the gas flow stops, then close the argon valve on the top of the bottle, and watch your argon meter. It should stay the same, if it slowly starts to go down, then you have a leak in your line and you need to check all your fittings and hoses to make sure they are tight and not leaking. If your argon line leaks bad enough, then it will start to do all sorts of weird things, and you'll be very frustrated trying to get a good weld going.
    -------------------------------------------
    Spike Customs, Inc.
    Fresno, CA 93727
    ph- 559-549-RIDE(7433)
    -------------------------------------------
    -Follow me on twitter!-

  7. #7

    Default

    If the regulator came with the unit watch out a lot of them are liters per min instead of cubic feet per hour. I know that the Everlast regulators are in metric units. If it is you can look online for a conversion and them just write the conversion in magic marker on the glass.
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Everlast PowerPlasma 70
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

  8. #8

    Default

    Any chance you could post a video of the problem?
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

Similar Threads

  1. Off to a bad start...
    By WitchHunter in forum Pre-sales, Sales and Shipping questions
    Replies: 4
    Last Post: 05-30-2012, 07:58 PM
  2. arc start problem.
    By Ram48 in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 13
    Last Post: 12-24-2010, 02:08 AM
  3. 250 ex arc wont start
    By johnson697 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 18
    Last Post: 05-26-2010, 03:40 AM
  4. HF start?
    By jtybt in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 5
    Last Post: 01-20-2010, 12:17 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •