    I have been welding in different jobs since 1999. Custom exhaust, machine building, Pharmacutical piping and machinery. I am Not certified in any form of welding (except orbital welding, but to me it doesnt count cause I mostly push buttons). I have been lucky enough to not need it.
    So the following is my OPINION of the Micro 185.
    I will start with the bad.
    The torch:
    A little big for my taste. My hands are about average size and I had a real hard time pencil holding the torch while welding some smaller stuff. I found it nearly imposible to activate the switch from this grip as well. It worked fine while welding bigger stuff in fillet welds and a normal grip.
    fit of the included collets was very rough. Tungsten did not slide in and out easilty at all. I ordered a weld craft torch last nite and I am anxiosly awaiting its arrival.
    The pedal:
    Crap. Rough opperation. Came inopperative from factory. Had to do some tweeking to get it to work. I dislike it completely. At least it was cheap.
    The Good.
    I can tell right away this welder is going to be just what the doctor ordered. Seems well built. Opperation is simple and straight forward. Perfect for home/hobby use. Low amperage was outstanding! I was welding some stainless steel trays for a local diner last nite and had it turned down to 6 amps. I suspect it is actually welding a bit higher that that due to it blowing thru some .030 sheet a bit fast. But was fine once I adjusted my timing. AC hasnt been tested yet but I will report as soon as I do. All in all a fine machine so far. Cant speak on longevity yet but I have high hopes.
    Kenny

  2. #2
    Join Date
    Feb 2011
    Location
    Fridley, Minnesota
    Posts
    376

    Default

    I just got one too, and I've only welded aluminum with it. I agree that the stock torch is quite the handful. I'm going to order a small male to large female DINSE adaptor so I can try the machine out with my WP20 water cooled setup. So far, I'm impressed at the performance of such a small machine, at such a small price. I'll try some thin gage stuff as soon as time allows. What size tungsten were you using?
    "It's not magic it's experimental, kind of like washing your hands after pooping used to be." -House

    Everlast PowerTig 250EX-arrived 1-26-2012
    Everlast PowerCool W300-arrived 1-26-2012
    Everlast PowerTig 185 Micro-arrived 1-26-2012
    Everlast PowerPlasma 70-arrived 1-26-2012
    ESAB MigMaster 250-borrowed
    HyperTherm 151 AKA "The Light Sabre"
    Linde UCC-305-964 lb. of old time water cooled TIG love-SOLD-Bad MOJO
    Purox OXY/ACETYLENE

  3. Default

    Quote Originally Posted by hooda View Post
    I just got one too, and I've only welded aluminum with it. I agree that the stock torch is quite the handful. I'm going to order a small male to large female DINSE adaptor so I can try the machine out with my WP20 water cooled setup. So far, I'm impressed at the performance of such a small machine, at such a small price. I'll try some thin gage stuff as soon as time allows. What size tungsten were you using?
    I am in the process of changing to the WP17. I failed to realize that the adapter (Q5g-150) has a DINSE 50. Now I need the small male to large female adaper.
    What a pain in the ###.

  4. Default

    Being that you likely purchased the unit in the USA i am not sure what pedal would be supplied or even if you have the WP17 torch with this unit.
    I find the foot pedal i have with the units while certainly not top of the line still they are decent enough. The WP 17 torch is a little smaller than the 26 ( not sure but i think you have this model)
    but it is still a little bulky. We will likey be looking at options for torches this coming year and will be seriously looking at changing these for the future.
    Cheers
    Duncan
    Last edited by Titan winch; 02-07-2012 at 01:48 AM.
    EVERLAST CANADA
    www.everlastwelders.ca
    www.titanwinches.com

    905 637 1637

  5. #5
    Join Date
    Dec 2011
    Location
    Kansas City Missouri
    Posts
    11

    Default

    I got my micro 185 in december it came with the wp26. I agree the torch which came with the welder is quite a handful. I'm in the process of building a water cooler and going to a wp20 water cooled torch. I got the slwhat 25 adapter from arczone it connects the welder and torch power/water cable perfectly. I machined my own adaptors for the argon and water hoses.
    Last edited by vettebob; 02-09-2012 at 02:30 AM.
    Lincoln 180 Mig 36inch blast cabinet
    Grizzly 10x22 Lathe 12 Ton hydraulic press
    Enco Square column Mill
    Oxy Acetylene Torch
    Power Plasma 50
    Micro Tig 185

Similar Threads

  1. MTS250 first impressions
    By TheGary in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 6
    Last Post: 07-26-2015, 01:02 PM
  2. iMig 140E First Impressions
    By Slartybartfa in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 6
    Last Post: 02-08-2015, 06:34 PM
  3. SuperCut 50P first impressions
    By kencal51 in forum Everlast Plasma Cutters (PAC)
    Replies: 0
    Last Post: 10-29-2012, 12:36 AM
  4. MTS 200--Some First Impressions
    By jackw19 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 4
    Last Post: 12-18-2011, 04:41 AM
  5. New 225LX first impressions
    By Mikey B in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 05-13-2011, 12:34 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •