i've got a supercut 50 and it stopped cutting. when you push the button the air comes on but it will not arc. if you loosen the electrode a little it will spark but will not cut. I opened up the machine but could not see any thing blown. the air pressure is 60psi. it worked perfect but just quit suddenly. i changed the tips but nothing still works and the ground is ok. any ideas.