If you have a 25' or longer torch lead, should it be uncoiled when welding ? Just wondering if the magnetic field would cause problems.
If you have a 25' or longer torch lead, should it be uncoiled when welding ? Just wondering if the magnetic field would cause problems.
Links to my welding projects > : Spray Arc with the 250p : Coldsaw Stand : Welding Cart : Heavy Duty Rolling Shelf : Taller Bandsaw
2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw
I worked with an electrical engineer for a long time and learned a few things. This is my opinion but as long as the leads are away from the piece you are welding the field should not be a problem. I would not leave the coiled next to the welder though. I would think it could over time mess with the electronics. I have heard of people the welding magnetised pipe wrapping the ground lead around the pipe to offset it. I have never done this so I wouldn't know if it works. One thing for definite though when we used a amp probe and we had to measure a wire with a low current we would wrap the wire around the clamp 10 times and that would magnify the reading by ten times. So one amp would be 10 amps on the meter for more accuracy. So every time a wire is coiled it is adding another set of amps. If you had a wire wrapped 5 times and welding at 100 amps the field would equal 500 amps. Ten times would be 1000 amps. I would not like to weld around that field all day. I cringe when I see welders wrap the lead around there arm a few times. Look up inductance heaters online. The can boil copper without ever touching it. Just the electromagnetic field melts the copper. So sorry for the long rant but that it my opinion.
Everlast PowerTig 250EX
Everlast PowerCool 300
Everlast PowerPlasma 70
Lincoln Powermig 215
Magnum SG Spool Gun
Don't jump on my Gomba
While a coiled lead will create a magnetic field, it will not heat up your arm if you put it through the center. If you put a magnetic, or paramagnetic material inside the field, flow will be induced in the material that is inside the coil. The magnetic flux inside the material inside the coil will have eddy currents in it which will internally heat the material. These eddy current losses can create quite alot of heat, especially at high frequencies, enough to melt the material in some cases.
While the coil may or may not have an impact on teh electronics, wrapping it around your arm won;t cause it to heat up, unless you have a metal rod in it. That said, there is likely some small amount of radiation being emitted by the wire that, over time may do something.
Everlast 200DX
Everlast PT185
Shoptask 3-in-1 (not currently in my garage, but I own it...)
Any day on a motorcycle like this that ends just needing parts and labor is a good day.
4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile
Inductance heaters usually also switch much faster than your welding AC waveform, which maxes out around 240Hz. If you switched it fast enough, with your arm in the middle, it WOULD cook it. That's how a microwave works. The frequency depends on the magnetic permeability of the material.
Optimal heating happens when you are basically pushing the material you are trying to heat right up the saturation point. This is why you can switch slower for larger pieces. They can handle a lot more magnetic flux before saturation. Once the material saturates, then trying to induce more flux with more current or more duration will be useless. So, you reverse the polarity and go the other way. Back and forth, back and forth. The hysteretic and eddy losses heat up the material.
This is the EXACT same principle (but essentially in reverse) that allows the same amount of current from a smaller transformer in an inverter welder. A older style transformer welder needs a huge transformer, because it's confined to switch at 60Hz. It needs a core that can handle a LOT of flux to transfer the power without saturating. However, an inverter welder switches must faster, and its core can be much smaller.
If you allow a magnetic material to saturate, it stops acting like a magnetic material. This is BAD NEWS BEARS in transformer and inductor world. A transformer looks not like a transformer, but more like a dead short. Same goes for an inductor. Now imagine saturating a transformer that was connected to 220V mains. Now you can see why they are so big.
Now, if you coil your welding leads, you form a nice little air-core inductor. The inductance will be so small that it most likely won't do anything. It will, however, broadcast all SORTS of switching noise. Since your inverter welder has a PWM switching overlay to control the current, even in DC, that switching frequency is most likely getting radiated, depending on the filtering in the machine. I don't know what the frequency is for everlast. Most likely just above 20kHz, so it doesn't drive you nuts with a high pitch whine.
Vice Grips
WD-40
Duct Tape
A coiled lead will heat up over time, but it would take a while! My parents remodeled a house that caught on fire. The guy left one of those extension cord shop lights on while he was on vacation. He left it coiled up with the light on, and from what I understand that creates a transformer. It took about 4 days but it finally generated enough heat to catch on fire.
Lincoln Eagle Engine Drive
Everlast MTS 250
Everlast Power Tig 225lx
HTP Mig 2400
Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
Miller Spectrum 375 Extreme Plasma cutter
Victor cutting torch
HF 20 Ton Shop Press
HF 4x6 Band Saw
HF Air Compressor
Northern Tool Drill Press
www.murphywelding.com
Hmmm? Never heard of any of this but I usually have my lead uncoiled and stretched out on the floor but this is usually for making moving around easier. If I'm sitting at the table welding I sometimes only uncoil what I need to reach the table. I always uncoil the MIG lead completely just to aid the wire moving inside the conduit .
I have read that having your torch lead coiled up can interfere with HF arc starting. Ever since I read that, I ALWAYS uncoil the torch lead completely and keep it away from my body as much as possible. Try not to put yourself in between the torch and ground cables. Not that it will kill you on the spot, just a precaution that will keep you out of the field. Can't hurt.
"It's not magic it's experimental, kind of like washing your hands after pooping used to be." -House
Everlast PowerTig 250EX-arrived 1-26-2012
Everlast PowerCool W300-arrived 1-26-2012
Everlast PowerTig 185 Micro-arrived 1-26-2012
Everlast PowerPlasma 70-arrived 1-26-2012
ESAB MigMaster 250-borrowed
HyperTherm 151 AKA "The Light Sabre"
Linde UCC-305-964 lb. of old time water cooled TIG love-SOLD-Bad MOJO
Purox OXY/ACETYLENE
As a side note, If you experience problems with arc blow in stick or arc wander in TIG, the cables can be coiled around the table leg, to help solve the issue. It's rare, that you'll get arc blow, but sometimes if the tig arc is bouncing around in the root, the magnetism of the metal particularly on a knife edge can destabilize the arc and make it wander. To get the arc to stabilize, it may take a little experimentation, and searching for the right "leg" to wrap it around, but it can help out somewhat.
Mark
performance@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x204
M-F 9am - 5pm EST
zoama585 I was wondering how you like the powerpro 256. I was torn between that and the powertig. Ultimately I went with the powertig because for the lift arc. I will be welding around sensitive car electronics. I know it's a million to one that it would fry a computer but I don't even want to take the chance. I work with some performance cars and the computers get programmed by laptop so the cars computers are expensive.
Everlast PowerTig 250EX
Everlast PowerCool 300
Everlast PowerPlasma 70
Lincoln Powermig 215
Magnum SG Spool Gun
Don't jump on my Gomba
Links to my welding projects > : Spray Arc with the 250p : Coldsaw Stand : Welding Cart : Heavy Duty Rolling Shelf : Taller Bandsaw
2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw
I'm very jealous I want the I-Mig250p. It looks like a very serous machine. I bet it can spray transfer very well.
Everlast PowerTig 250EX
Everlast PowerCool 300
Everlast PowerPlasma 70
Lincoln Powermig 215
Magnum SG Spool Gun
Don't jump on my Gomba
@SeanMurphy265 I would be willing to bet that the heat generated was from the wire acting as a heating coil and not from the electromagnetic field.
Everlast lx225
Hobart Handler 210 with spool gun
Hobart Stickmate LX
Thermal Arc 400GMS
40 amp Northern Tools plasma torch
130 chicago electric tig welder
90 amp chicago electric flux mig
10"-22" Grizzly lathe
15"-5.5" Grizzly vertical end mill
In need of nice TIG machine. drooling over PowerTig 250ex