    Are there smaller tips than 1.0 for the A81 torch? We have been using an old Matco plasma with I think 12.5 to 20 amps and .6 to .8 tips to cut off quarter-panels and such.

    The 70 amp plasma cutter with a 1.0 tip is overwhelming for cutting off quarter panels. Would a smaller torch that is designed for a 20 amp plasma with smaller tips make this big plasma cut more like the smaller machines do on thin sheet-metal?

  2. #2

    Default

    if you go to fitamet site ,they only list 1.2 and 1.0`s tips, i`ve cut sheetmetal with both 1.2 and 1.0 tips, the 1.0 does a clean knife cut when set corectly
    Gil
    powerpro 256
    lincoln 185

  3. #3

    Default

    I'd suggest looking at the PP50, instead. It'll handle a lot of different ranges as well. The s-45 is pretty good on thinner stuff.

Similar Threads

  1. much smaller torch for powerpro 256?
    By acannell in forum General Welding Questions
    Replies: 53
    Last Post: 08-12-2014, 11:21 PM
  2. Change tig torch to a smaller water cooled torch
    By wheelrdealer in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 4
    Last Post: 09-18-2012, 05:07 PM
  3. Looking to get smaller torch soon, what do you recommend?
    By Mark in forum TIG Welding (GTAW/GTAW-P)
    Replies: 12
    Last Post: 11-25-2011, 09:34 PM
  4. Replies: 14
    Last Post: 08-30-2011, 07:32 PM
  5. Switching to a smaller tig torch?
    By Legacyartist247 in forum General Welding Questions
    Replies: 3
    Last Post: 07-25-2011, 06:46 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •