    Just for kicks I was "Trying" to weld .020 thick stainless using 18-20 amps.
    While welding I noticed the HF struggled to start the arc. Is this a normal thing
    at 20 amps? I used 1/16 thoriated tungsten.

    I gave up, I was more or less burning holes thru the material.
    Brian Scott
    225LX
    Speedglass 9002v helmet
    19" Shop Fox band saw
    Ingersoll Rand air compressor

  2. Default

    Was the pre flow on?

  3. #3
    Join Date
    Jun 2011
    Location
    Charleston, South Carolina
    Posts
    50

    Default

    Quote Originally Posted by Buggy Chief View Post
    Was the pre flow on?
    Yep! Pre-flow was set at 1 second
    Brian Scott
    225LX
    Speedglass 9002v helmet
    19" Shop Fox band saw
    Ingersoll Rand air compressor

  4. Default

    That will delay the arc start. Gas starts flowing to shield the tungsten b4 there arc starts. If you want an immediate arc, then turn pre flow on 0.

  5. #5

    Default

    Not sure if he was talking about the pre flow - it sounded like the arc just did not like to start.

    Brian?

    Cheers,

    Mike

  6. #6

    Default

    On very low amps you have to keep a tight arc and sharpen the tungsten to a sharp point. I have gotten my powertig 250ex to keep an arc going at 6 amps.
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Everlast PowerPlasma 70
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

  7. #7

    Default

    Did you have any luck with the arc? Like I said at low amps you have to sharpen it to the point it could draw blood from you. Also you could try polishing the tungsten with fine fine wheel. Don't use sandpaper though.
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Everlast PowerPlasma 70
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

  8. #8
    Join Date
    Jun 2011
    Location
    Charleston, South Carolina
    Posts
    50

    Default

    Quote Originally Posted by Cippee View Post
    Did you have any luck with the arc? Like I said at low amps you have to sharpen it to the point it could draw blood from you. Also you could try polishing the tungsten with fine fine wheel. Don't use sandpaper though.
    That helped! I got it to work. It's just a fine line how close the tungsten
    is to the work piece.
    I think I need more practice.
    Brian Scott
    225LX
    Speedglass 9002v helmet
    19" Shop Fox band saw
    Ingersoll Rand air compressor

  9. #9

    Default

    That's good. Yeah at lower amps there is less current to overcome a larger gap so it is more sensitive to a larger arc gap then at 100 amps.
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Everlast PowerPlasma 70
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

  10. #10

    Default

    I don't know if you would see a difference, but I have always had better luck with the ceriated electrodes. I could even get my lift-start tig to fire off at 5 amps, although having it needle sharp makes a much bigger difference.
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  11. #11

    Default

    Did you get it needle sharp by hand or use a powered sharpener?

  12. #12
    Join Date
    Jun 2011
    Location
    Charleston, South Carolina
    Posts
    50

    Default

    Quote Originally Posted by Mike J View Post
    Did you get it needle sharp by hand or use a powered sharpener?
    No. I used a power sharpener.
    Your saying I should hand grind and then
    polish to remove the small grind defects?
    Brian Scott
    225LX
    Speedglass 9002v helmet
    19" Shop Fox band saw
    Ingersoll Rand air compressor

  13. #13

    Default

    Oh no, I am just curious - new to TIG, and am interested in low-amp work, I may need it for some of the project i am thinking about.

    So far, with the welding I have done, and the courses taken, its all been hand ground, using on a diamond stone. I can understand if you want accuracy, it's much better to use a power sharpener. I may get one of those....

    Cheers,

    Mike

  14. #14

    Default

    I like lathinated 2% they are hard to find but work better than anything else. Most places only have 1 1/2% lathinated whitch done work nearly as well.
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Everlast PowerPlasma 70
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

  15. #15

    Default

    Quote Originally Posted by Mike J View Post
    I can understand if you want accuracy, it's much better to use a power sharpener. I may get one of those....

    Cheers,

    Mike
    I was dangerously close to dropping three hunderd on one of those, then I tried my 4" diamond wheel grinder (I use on tile) clamped in the vise, electrode in a drill, that cured me. Wheel is about $25.. Those grinders look nice, but they're definitely a rip off.. there has to be 20 times the diamond on a 4" wheel, much straighter longitudinal cut too, from bigger diameter.
    Last edited by Jake98; 02-12-2012 at 05:00 PM.
    Everlast PowerPlasma70
    Hobart Ironman 230
    Lincoln A-D/C 225
    'Classic' Everlast Powertig 200DX 'We don't need no steenkin pre-flow..'
    jakemateer.com

Similar Threads

  1. Surge amps
    By Chevelle69 in forum General Welder Questions
    Replies: 2
    Last Post: 02-17-2015, 07:44 PM
  2. amps req. for .095 aluminum
    By backhoe in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 12-05-2011, 04:39 PM
  3. 250 ex 250 amps ac
    By jdt1986 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 07-09-2011, 10:51 PM
  4. PT 250 EX stuck at 478 Amps!!!
    By Jetfire3 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 06-10-2011, 03:33 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •