dyethor Project #3 Dyethor, Pipe... 02-20-2012, 03:22 PM
dyethor Here is a close up of the... 02-20-2012, 03:28 PM
jp2code That's a nice looking bead! ... 02-20-2012, 05:05 PM
Powertig great looking tool I wasn't... 02-20-2012, 11:15 PM
dyethor Thanks. The beads are still... 02-20-2012, 11:36 PM
redbeard Very nice solution to the... 02-21-2012, 05:56 AM
dyethor Yea, its nice not being... 02-21-2012, 01:44 PM
Previous Post Previous Post   Next Post Next Post
  1. #1

    Default Project #3 Dyethor, Pipe flange tool

    Hello all.
    This is project is a pipe flange tool. Its for wrenching on flanges that are welded to pipe with NPT threads that go into various equipment. I came up with this design out of necessity. Previously I had been either using a large pipe wrench or a strap wrench. The pipe wrenches would always leave gouges in the soft aluminum pipe, to me that's unprofessional looking and not how I do work. Using a strap wrench was a pain to get good torque and was difficult to use in smaller places.

    I Built this tool out of stainless I had laying around.. The handle is 1" square tubing 1/8" thick. The Pin's are made from 3/8" round bar.


    Here is the tool. The two pins that are close together are 2" long. The one on the end is 3". I drilled holes through the square tubing that were pre-measured to the correct spacing to fit on the flanges. Then I tig welded the pins in place.
    Power tig 225lx
    Hand tools up the wazoo.

  2. #2

    Default

    Here is a close up of the orientation of the pins to the flange on a 2" and 3" pipe flange.


    Here is a 4" pipe flange. I only have one prong go into the bolt hole the other presses on the outside of the flange. The flange is and example of some of my aluminum tig welding.


    I use the prong on the opposite side to hook in a flange, then use the pipe as a leverage point. sometimes there isn't enough room access the face of the flange.

    Here is a picture of the too.
    Here is an example of the area the tool would be used in. If you look there is an engine on the left side its connected to a pump. On top of that pump is a nice blue flange/pipe screwed into the pump.
    Power tig 225lx
    Hand tools up the wazoo.

  3. #3

    Default

    That's a nice looking bead!


  4. #4

    Default

    great looking tool I wasn't quite able to figure out how you use it but I get the gist. I am sure it does the job well. it's great to see that you took the time to create a solution that gives professional results. If your capable of welds that look like that, the last thing you want is gouges just down the pipe.
    Miller Challenger 172 Mig
    Soon to be winner of a Powertig 210 EXT

    Wade Mortenson

  5. #5

    Default

    Thanks. The beads are still not as consistent looking as I want but I'm working on it. As far as the gouges go. I want everything to look good on the tankers when the D.O.T. officers pull our trucks over and give inspections.
    Power tig 225lx
    Hand tools up the wazoo.

  6. #6
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Very nice solution to the problem. Isn't it great to have the ability to make custom tools?
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  7. #7

    Default

    Yea, its nice not being limited to only buying tools that don't do the job proper.
    Power tig 225lx
    Hand tools up the wazoo.

Similar Threads

  1. Project #4 Dyethor Gasoline processing table
    By dyethor in forum Heavy Equipment and Commercial Projects
    Replies: 13
    Last Post: 03-09-2012, 03:54 PM
  2. Project #5 Dyethor trade show display
    By dyethor in forum Heavy Equipment and Commercial Projects
    Replies: 12
    Last Post: 02-27-2012, 04:53 PM
  3. Project #1 Dyethor Control panel box.
    By dyethor in forum Heavy Equipment and Commercial Projects
    Replies: 18
    Last Post: 02-24-2012, 05:44 AM
  4. Wastegate Flange Project
    By scootarida1 in forum On Road Fabrication
    Replies: 4
    Last Post: 12-29-2011, 03:31 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •