Share
Results 1 to 15 of 15

Thread: My new 225lx

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Default My new 225lx

    My welder just got here via the big brown van. Opened up the box, no shipping damage. Hooked up all the hoses. Put a 50amp plug on the power cable. The following picture are some test welds playing around with the settings.


    Just a question is the fan supposed to run the whole time? As soon as I turned the power on it started running.

    Now I'm off to build my first project.
    Power tig 225lx
    Hand tools up the wazoo.

  2. Default

    I've got a 200 and the fan starts when I flip it on, I'm assuming yours is the same. Based on what I've read in other posts that's the way they're set up. Keeps it nice and cool but it is a bit noisy :-)

  3. #3

    Default

    Oh man I'm sorry to hear that. I was welding one day and when I stopped I realized my niece was watching me for the last 30 sec from what I could gather. I didn't even know they were over I was so worried that she had hurt her eyes. She is only 4 so she didn't know it was bad to look she just wanted to say hi. Luckily I was only welding at about 30 amps and she didn't hurt her eyes.
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Everlast PowerPlasma 70
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

  4. #4

    Default

    I believe the fan is suppose to run the whole time. Its not a fan-on-demand setup
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  5. #5

    Default

    Yea. I've done some research and came to that same conclusion.
    Power tig 225lx
    Hand tools up the wazoo.

  6. #6

    Default

    That's the reminder that the unit is still turned on.

    Its not a bug; its a feature!

  7. #7

    Default

    Quote Originally Posted by jp2code View Post
    That's the reminder that the unit is still turned on.

    Its not a bug; its a feature!

    Good one ..
    Oleg Gladshteyn
    Phone: 650 588 8082 / 877 755 WELD
    Cell: 415 613 6664 ONLY IF YOU REALLY NEED IT
    Email: oleg@everlastwelders.com
    Website www.everlastgenerators.com

    www.linkedin.com/pub/oleg-gladshteyn/48/b08/875

  8. #8

    Default

    Quote Originally Posted by welderdude View Post
    I believe the fan is suppose to run the whole time. Its not a fan-on-demand setup
    By having fan on all the time , we get better duty cycle out of the unit
    Oleg Gladshteyn
    Phone: 650 588 8082 / 877 755 WELD
    Cell: 415 613 6664 ONLY IF YOU REALLY NEED IT
    Email: oleg@everlastwelders.com
    Website www.everlastgenerators.com

    www.linkedin.com/pub/oleg-gladshteyn/48/b08/875

  9. Default

    I actually like the fan on all the time. Its not loud at all. I dont even hear it running. I usually have the radio on anyways. Also ya have less to go wrong, higher duty cycle and its quieter than my old lincoln which is on all the time too.
    Gabe
    everlast power arc 200
    Lincoln electric 225 tombstone
    lawn mowers

  10. #10

    Default

    I like the fan being on all the time myself. Looks like your off to a good start!
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  11. #11

    Default

    I'll get use to the noise. I'm use to a quiet shop, since its only me.

    So far I like this welder it has an easy user interface. I'm not use to a flow meter with liters per min that will take a little time to get use to tuning for different things.

    So I dropped a piece of steel onto my foot pedal cord, it cut through it in two pieces. I will have to make some splices tomorrow. I didn't want to break my groove so I tried out the torch button. So far I like it. The only problem is since I'm not use to having a button on the torch I accidentally hit it in 4t and got arc flash to my face and eyes. This is the first time its been this strong. right away I could smell a little toasty skin. I was about 1.5' form the arc. My face is a little toasty, my eyes are throbbing and I have a headache. And my vision has a big spot and is a little blurry. That is a touchy switch.
    Power tig 225lx
    Hand tools up the wazoo.

  12. #12

    Default

    It might not be a bad idea to go get it checked out if your seeing a spot.
    They may want to use some antibiotics and patch them.

  13. #13
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by dyethor View Post
    I'm not use to a flow meter with liters per min that will take a little time to get use to tuning for different things.
    geezer posted up a nice rule of thumb on that not too long ago, flow in lpm should be equal to the cup size, 1 or 2 less for a gas lens, +1 for higher amps (200 or more IIRC)
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  14. #14
    Join Date
    Oct 2011
    Location
    Litchfield Park, AZ
    Posts
    370

    Default

    If you are use to using a Miller with fan on demand, the constant fan noise it is a change at first. I do not desire the fan to be on all the time but the initial irritation has gone away for myself and I do not even notice it is on much when I start welding.
    Miller 252
    PowerTig 250 EXT
    Evolution Rage 2
    48X6 inch Belt Sander w/ 9 inch Disk Sander
    ...

  15. #15
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    I remember I was doing little tack welds once without my helmet, just blinking my eyes shut and firing a brief high-amp arc, to make small tack welds. I did do quite a few of them - 20-40 or so and high amps (but brief.) I ended up sunburning my face on that!

    After that painful experience, I haven't skipped out on the helmet (even for just those really quick tack welds.)

    My super200P has its fan on all the time with the power on, but it's a pretty mellow noise. Really moves the air through the vents too...
    Last edited by jakeru; 02-24-2012 at 07:03 AM.
    '13 Everlast 255EXT
    '07 Everlast Super200P

Similar Threads

  1. 225lx??
    By THUNDER351 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 04-20-2012, 07:38 PM
  2. 225LX can't seem to get it to tig..
    By Hayapower in forum TIG Welding (GTAW/GTAW-P)
    Replies: 19
    Last Post: 12-10-2011, 12:57 AM
  3. Just got my 225LX and tried it out
    By DiabolicZ in forum TIG Welding (GTAW/GTAW-P)
    Replies: 29
    Last Post: 04-02-2011, 08:01 PM
  4. my new 225lx
    By paintmegone in forum Customer Testimonials
    Replies: 1
    Last Post: 06-15-2010, 05:23 PM
  5. 225LX on the Way !!!
    By alexm in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 02-16-2010, 11:19 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •