Originally Posted by
Farmer
Sorry got pulled away from computer before I could finish ... Read out will run from minimum setting 19 amps to about 22 amps as you increase the power setting then jumps to 49 amps ( from about the 1/2 way point on the power dial to the maximum setting it never changes just reads 49 ) I have had a chance to try cutting with it and it seems that it will go to the minimum setting and maximum only . I tried cutting some 1/2 inch flat stock on the 22 amp setting and it would not cut thru ( 18 gauge was fine ) Turned the power dial to the 1/2 way point ( read out is at 49 amps ) and it will cut 1/2 inch stock .
It appears it only has the ability to produce the lowest power setting and the maximum power setting. Has worked flawlessly till now hope it is an easy fix ( purchased it in Aug of 2010 )