Share
Results 1 to 8 of 8

Thread: UpPipe For a Rotated Turbo Subaru Forester

  1. #1

    Default UpPipe For a Rotated Turbo Subaru Forester

    The up pipe is made out of 2.25" 11 gauge mild steel and I choose to have a long smooth bend in order to maximize flow and hopefully help with spooling the turbo. The turbo is going to be a AGP/Borg Warner S261.







    That isnt the turbo I am going to be using it was just used to picture how it will sit.













    I am also making a clear hood scoop delete so that way you can see into the engine bay.
    I sandblasted the pipe and am currently in the middle of coating the pipe with VHT Flameproof.
    Brandon Raineri
    The Pennsylvania State University
    Studying Industrial Engineering

    Everlast PowerPro 205
    Everlast I-Mig 200
    SpeedGlas 9100x
    Milwaukee 14" Dry Cut Saw
    Craftsman 6"x48" Belt Sander with 9" Disc Sander

  2. #2

    Default

    Will you port and polish the heads and intake? With stock heads and intake how much air flow can you have?
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  3. #3

    Default

    Quote Originally Posted by SeanMurphy265 View Post
    Will you port and polish the heads and intake? With stock heads and intake how much air flow can you have?
    Usually no need to do anything to the heads unless you are really trying to push it. Stronger valve springs maybe if the boost is going to be significant, but it probably isn't going to be very high boost on that application.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  4. #4

    Default

    Yeah I probably wont port the heads. I will be running moderate boost of 18-20psi which is normal since it was already a turboed vehicle. Eventually I will probably build the heads and such.
    Brandon Raineri
    The Pennsylvania State University
    Studying Industrial Engineering

    Everlast PowerPro 205
    Everlast I-Mig 200
    SpeedGlas 9100x
    Milwaukee 14" Dry Cut Saw
    Craftsman 6"x48" Belt Sander with 9" Disc Sander

  5. #5

    Default

    Those things are factory turbo'd? I didn't know they had a turbo option for those.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  6. #6

    Default

    Where I grew up we have an Air Force base in our town. One of my friends worked there mowing all summer. This family had an older Subaru wagon 4x4 for sale, and my buddy bought for $130.00 because they were getting shipped over seas. They could not kill that car! They jumped and would get 6 feet of air over and over again. They ran it through a creek in 2-3 feet of water, and never killed that car. It got to be a running joke about what they could do to that car to kill it. At the end of the summer they cut off the roof and made a convertible. I think someone gave a $100.00 for it. That car was an absolute beast!
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  7. #7

    Default

    Thats what I have heard, unfortunately these cars do not like when you push the boost to much on them. I have a feeling the engine is going to come out next year to be built. Hopefully I will have some funds so I can build it before it blows and not risk damaging the block or heads.
    Brandon Raineri
    The Pennsylvania State University
    Studying Industrial Engineering

    Everlast PowerPro 205
    Everlast I-Mig 200
    SpeedGlas 9100x
    Milwaukee 14" Dry Cut Saw
    Craftsman 6"x48" Belt Sander with 9" Disc Sander

  8. Default

    Boost, Timing, static Compression.

    Pick two.

    I helped in preparing Colin McRae and Travis Pastrana's Sobe Gold X Games 10 cars.

    Vermont Sports Cars built the car, and we had a 4wd dyno for tuning at F1Dyno in Portland, Me.

    They hired a Guy from Autech Engine management in Australia, he did all the tuning, even start-up maps.

    The timing was around 38* @ WOT, which is crazy dangerous even on 100octane.

    He was explaining that because the Two halves of the EJ case that wrap around the crank centerline actually stretches, so the crazy timing advance was to "Baseball pitch" the spark into the Combustion chamber.

    This is the type of tuning that would normally melt an engine, but those guys in Aus know whats up!

    You can't make this stuff up. This guy was so smart, I felt like I learned 2 yrs of college in 2 hours!
    Spec-C Tuning and Fabrication

Similar Threads

  1. Cummins turbo mount
    By dzljon in forum TIG Welding (GTAW/GTAW-P)
    Replies: 34
    Last Post: 10-28-2017, 07:03 PM
  2. 2007 Subaru STI - Weekend Warrior
    By alcoolaid in forum Truck, Car and Bike builds
    Replies: 24
    Last Post: 06-23-2014, 02:51 AM
  3. Turbo Oil Catch Can
    By scootarida1 in forum On Road Fabrication
    Replies: 4
    Last Post: 06-26-2012, 07:55 PM
  4. Project 1, from scootarida1, My 2005 Subaru Forester XT Turbo Project
    By scootarida1 in forum On Road Fabrication
    Replies: 11
    Last Post: 08-19-2011, 02:32 AM
  5. New Turbo Header for my bike
    By sportbike in forum On Road Fabrication
    Replies: 12
    Last Post: 05-22-2011, 02:01 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •