Share
Results 1 to 5 of 5

Thread: Pu 205 questions please

  1. #1

    Default Pu 205 questions please

    Hi, I'm finally getting around to practicing with my pu205. I have two questions:
    1) when I was using the plasma cutter, after a cut, the air wouldn't quit coming from the nozzle until I turned the machine off and start over again?

    2) I'm practicing with my tig using the foot pedal:
    A) I can't set the amperage, or I'm doing something wrong. I was trying to set the amperage to, say 50 amps max, but it still goes to max despite the machine being set at its lowest amp. However, the display reads -006, doesn't go to zero, is it supposed to go to zero with the foot pedal let off?

    B) the argon keeps flowing after I let off of the pedal, unless I turn the machine off. Argon is going quickly at this rate. Yikes!

    Thought I'd try here before calling tech; )
    Dne'



    My work area for practicing, pretty cool?
    Last edited by Dne007; 03-13-2012 at 04:48 PM. Reason: Photo added

  2. #2

    Default

    Darn, just tried calling tech but their mailbox is full and I wasn't able to leave a message. : (

  3. Default

    Quote Originally Posted by Dne007 View Post
    Darn, just tried calling tech but their mailbox is full and I wasn't able to leave a message. : (
    does it continue for longer than the setting you have your post flow on?

  4. #4

    Default

    Quote Originally Posted by Dne007 View Post
    Darn, just tried calling tech but their mailbox is full and I wasn't able to leave a message. : (
    please will contact Ray at ext 207 .. VM issue is fixed now



    please
    Oleg Gladshteyn
    Phone: 650 588 8082 / 877 755 WELD
    Cell: 415 613 6664 ONLY IF YOU REALLY NEED IT
    Email: oleg@everlastwelders.com
    Website www.everlastgenerators.com

    www.linkedin.com/pub/oleg-gladshteyn/48/b08/875

  5. #5

    Default

    I only have about 2-300 pounds in my tank, but I checked the post flow. The knob wasn't on correctly, not that it makes any difference, but I pulled it off and put to "0". All n all, I think you solved my problem! However, the argon was shutting off just fine, then began to keep flowing the more I tigged. I wouldn't consider what I was doing excess excessive, just little pieces of thin scrap. Wow, Tech just called, and I had played with the post flow just before he called, and it seems to be working just fine for the tig. I'll work with the plasma tomorrow, ( with him on the line would take too long to swapfrom tig to plasma) maybe I overloaded the machine by cutting too much too quickly, like maybe taxed the duty cycle? I thank you!!!!!! and will have tank filled tomorrow and give both the tig and plasma cutter a little workout! I love my little machine and would fear for it to break!
    ; )
    Dne'

    Quote Originally Posted by fdcmiami View Post
    does it continue for longer than the setting you have your post flow on?

Similar Threads

  1. Questions About I-Mig 140
    By esg612 in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 16
    Last Post: 02-22-2017, 06:26 PM
  2. New guy with 250ex questions.
    By gree box in forum TIG Welding (GTAW/GTAW-P)
    Replies: 26
    Last Post: 01-29-2013, 10:11 PM
  3. 256 questions
    By tnc110 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 43
    Last Post: 05-02-2012, 01:03 PM
  4. spool gun questions
    By Ram48 in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 2
    Last Post: 10-25-2011, 01:34 AM
  5. 250EXT Questions
    By zoama in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 09-08-2011, 01:20 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •