Share
Results 1 to 8 of 8

Thread: Protection against a dust

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1
    Join Date
    Dec 2011
    Location
    RUSSIA.Sankt Peterburg
    Posts
    218

    Default Protection against a dust

    Hi All,
    For workplaces and shops with high dust pollution, for example, the grinding dust, many manufacturers the welding equipment recommend (as additional option) to use the dust filter.
    I work in enough dusty facility, from here and a question-
    whether it is necessary to me to make the filter on my рр256?
    On mine EWM pico 162 I use such ( buy there was no possibility, made myself)
    Ruslan
    EVERLAST Power Tig 255 EXT
    EVERLAST PP256
    PC300
    EWM Pico 162
    MERKLE mobimig 180K
    SELCO Genesis 352 pme

  2. #2

    Default

    Building your own pre-air filter should be okay, as long as , the intake surface is so large that it couldn't possibly plug up and restrict the air flow that cools the machine. Dust and sawdust are always a problem.
    Some of those lies people tell about me, are true

  3. #3
    Join Date
    Dec 2011
    Location
    RUSSIA.Sankt Peterburg
    Posts
    218

    Default

    Quote Originally Posted by geezer View Post
    Building your own pre-air filter should be okay, as long as , the intake surface is so large that it couldn't possibly plug up and restrict the air flow that cools the machine. Dust and sawdust are always a problem.
    I understand that it is necessary to watch the filter and on a regular basis to clean,
    Which I wish to do the filter very simple in service
    Ruslan
    EVERLAST Power Tig 255 EXT
    EVERLAST PP256
    PC300
    EWM Pico 162
    MERKLE mobimig 180K
    SELCO Genesis 352 pme

  4. #4
    Join Date
    Dec 2011
    Location
    RUSSIA.Sankt Peterburg
    Posts
    218

    Default

    Today has made the filter
    All works perfectly,
    electronics is protected
    Ruslan
    EVERLAST Power Tig 255 EXT
    EVERLAST PP256
    PC300
    EWM Pico 162
    MERKLE mobimig 180K
    SELCO Genesis 352 pme

  5. #5

    Default

    It will probably reduce the duty cycle some, which will probably create some early thermal tripping and slightly longer reset times, but it should keep everything internally cleaner...
    __________________________
    Everlast Power I-MIG 200
    Everlast PowerUltra 205P
    Everlast SM 200-N
    Thermal Dynamics Cutmaster 42

  6. #6

    Default

    Donor,

    !!!!! PLEASE Do not use that. That filter is way too dense and interferes with the free flow of air. Also the grating/mesh that holds the filter has significant obstruction and I'd guess it is at least 30% reduction from just that! Ours are not engineered to have any obstruction.
    The 256 has a low duty cycle as it is at max. You will damage the machine seriously.
    ANY air restriction is forbidden and will void warranty. You must keep 1 foot clearance from any obstruction additionally to provide maximum air flow.

    It's better to remove the cover occasionally and blow out the inside with an an air compressor, and and air gun/wand.
    Last edited by performance; 03-19-2012 at 10:51 PM.

Similar Threads

  1. Welder dust cover....Where are they?...Vote/Poll...Who's in?
    By wileyone123 in forum General Welder Questions
    Replies: 43
    Last Post: 09-19-2014, 05:42 PM
  2. Brown dust on side of steel TIG weld
    By johnnymg in forum TIG Welding (GTAW/GTAW-P)
    Replies: 19
    Last Post: 08-15-2013, 03:47 AM
  3. Cutting with no eye protection...
    By CGCINC in forum Everlast Plasma Cutters (PAC)
    Replies: 23
    Last Post: 08-10-2012, 04:42 PM
  4. Power Surge Protection ?
    By Rivets in forum General Welder Questions
    Replies: 12
    Last Post: 04-13-2011, 06:31 AM
  5. Protection light on PT225LX
    By DiabolicZ in forum TIG Welding (GTAW/GTAW-P)
    Replies: 10
    Last Post: 04-08-2011, 03:39 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •