Protection against a dust
Hi All,
For workplaces and shops with high dust pollution, for example, the grinding dust, many manufacturers the welding equipment recommend (as additional option) to use the dust filter.
I work in enough dusty facility, from here and a question-
whether it is necessary to me to make the filter on my рр256?
On mine EWM pico 162 I use such ( buy there was no possibility, made myself)
Ruslan
EVERLAST Power Tig 255 EXT
EVERLAST PP256
PC300
EWM Pico 162
MERKLE mobimig 180K
SELCO Genesis 352 pme