Hello all,

Since I just bought my 225lx I had the need to make it a little more portable than just lugging it around by the handle. I do a lot of side jobs out in the field, so I needed a cart that could be moved easily on different surfaces. Not just a nice concrete floor. I had seen a project somewhere that the person based their cart on a dolly, this following project is my take on this.
I Built this out of aluminum I had laying around the shop. This includes 2x3 channel, 1x1x1/8 square tubing, 2.5x.25 flat stock, and some 3/16 and 1/4 sheet. I also used some 1/2 inch bolts, stainless steel hangers, and ratchet straps. Every weld was made using my 225 tig machine.

I started this project by making the cylinder cradle. Its built for a 125cf tank. I didnt want to lug around anything bigger.
Here is the main supports and the arch, made from the 2x3 channel. They parts are fitted and waiting to be welded.


I welded the arch first.


The main structure that cradles the cylinder.


Here I made the base for the cylinder.


Next I welded on the 1/4 sheet For the floor plate.


Here is the base welded to the main structure.


For this cradle piece I got a piece on metal that would fit in my pipe bender. I bent it and then cut off the excess.