Thread: Is there anything welding wise that uses Nitrogen gas???

  1. #1

    Default Is there anything welding wise that uses Nitrogen gas???

    I have a donated bottle of Nitrogen. Besides filling tires what else is it good for??? Local welding store is calling it a rental tank. So when the tank is empty we are thinking of just dropping it off unless we can figure out a trade.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  2. #2
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Nitrogen cylinder valves are CGA 580, the same as argon and argon-CO2 cylinders. Can your LWS draw a vacuum on it, relabel it, and refill it with your preferred gas, if they won't trade it?
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  3. #3

    Default

    Quote Originally Posted by DaveO View Post
    Nitrogen cylinder valves are CGA 580, the same as argon and argon-CO2 cylinders. Can your LWS draw a vacuum on it, relabel it, and refill it with your preferred gas, if they won't trade it?
    No, This size tank is considered a rental tank. (I think a 200 or 250 CF pretty big) So if you walk in with it and you do not have a contract, they just take it as theirs. No swap, no refill, no nothing. My buddy picked it up at a garage sale and it is full. I guess the guy that had it owned a shop. He used it for cleaning out AC systems. Looks like he will lose the money he paid for it, but it wasn't much.

    I have been following the other threads about how different LWS handle tank sizes differently.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

Similar Threads

  1. I'm not so sure I'm sold on these yet....service or product wise....
    By Rickracer in forum Customer Testimonials
    Replies: 19
    Last Post: 12-22-2013, 02:44 PM
  2. First Welding Project - You guessed it... a welding cart
    By EmptyNester in forum Hobyist Projects
    Replies: 19
    Last Post: 10-12-2011, 03:30 PM
  3. Nitrogen instead of Argon
    By Mad-Dax in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 10-31-2009, 09:28 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •