New 205 observations--
This could take a CS call. The new 205 combo is a beauty but seems to run at a max of about 30amps with foot pedal all the way down.
DC, mild steel, amps all the way up, preflow one second, post flow eight seconds. Arc force seems to make no difference, pulse makes no difference in power but sure is cool. One thing I've never seen before is a change in the light. #13 is not near dark enough during brief periods of a second or so, but seems just right on start-up, but this is my first try with inverter TIG and with a auto helmet. Reverting back to a 25 year old hat and memories of welders past, I see a dim arc, then a 'zinc contamination' blinding flash or flashes that wipes out the vision of any puddle that might have started. Ground seems good, no magic smoke from the machine....
Mostly confused right now.
Ideas?