    Hi. I'm SeanM and I'm in Illinois, about 1.5 hours West of Chicago. I started with a 90 amp Harbor Freight flux core MIG, then the red 130 amp Harbor Freight TIG, and now I've stepped up to the i-Tig-200. I'm "improving" a 67 Cutlass Supreme Convertible (I don't want to say restoring). http://www.everlastgenerators.com/fo...ies/smile1.png
    So far I've practiced with 16 and 22 gauge mild steel, and the foot pedal will come next week. To move up from lift arc to HF start, pulse, slope up & down, adjustable pre & post flow, WOW! So much better.
    One question out to the other members - My HF TIG came with a WP-9V torch, and that's a lot lighter than the WP-26 torch that came with the i-Tig-200. Perhaps I could use my WP-9V torch with the i-Tig-200. For 1/8" and thinner it has enough capacity, but:
    1. No switch (I understand only an issue when not using a foot pedal)
    2. Dinse connector on the WP-9V needs an adapter.

    I think I found an adapter on eBay for the Dinse connector, and I've seen TIG torch switches, so I should be able to find a 7-pin connector and run a wire with zip ties on the torch, or maybe get a new sheath (I haven't really looked into that).

    Any suggestions for a lighter torch if I'm doing "thin" stuff (everyone has their own perspective, but I'm talking 1/8" or thinner), and/or has anyone adapted a WP-9V similar to what I'm thinking about?

    - Sean

  2. #2

    Default

    Welcome to the board and I myself am very new to tig so i cant answer your question. But there are a lot of guys on here that can. good luck.
    Everlast Power Tig 200DX
    Thermal Arc Fabricator 181I
    Giant Tech 4800X Plasma
    Glenn-Roberts Classic Buzzbox

  3. #3

    Default

    Several people have purchased torches from arc zone.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  4. #4

    Default

    I would go a WP-18 , with 200 amp you will want water cool if you ever want to weld something thick or need a lot of amps . I built my own cooler for my welder coast about 150 buck getting stuff on ebay to build cooler

  5. #5

    Default

    Quote Originally Posted by SeanMurphy265 View Post
    Several people have purchased torches from arc zone.
    I stopped dealing with them and took down any links I had posted due to terrible service and outright lying to me. The last torch I purchased was a CK 210 and beat az's price by more than $50.

    Quote Originally Posted by seanm View Post
    Any suggestions for a lighter torch if I'm doing "thin" stuff (everyone has their own perspective, but I'm talking 1/8" or thinner), and/or has anyone adapted a WP-9V similar to what I'm thinking about?

    - Sean

    I use a CK130 up to 150 amp... it's very light and the cable is as limp as cooked spaghetti. Also note CK torches are rated at 100% duty cycle in AC and DC where others are greatly reduced in AC http://www.everlastgenerators.com/fo...ad-on-my-PP256
    Last edited by zoama; 04-02-2012 at 02:44 AM.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  6. #6
    Join Date
    Mar 2012
    Location
    Remote S. Idaho
    Posts
    53

    Default

    A WP-9 works just fine with 1/16 tungsten and thin materials up to about 150amps. You'll feel it getting too hot to handle if you're asking too much of it. They're much lighter and easier to handle.
    There is no safe direction to point an unsafe gun.
    PowerPro 205
    Hobart 250HF
    Powcon 300ST
    gas stuff
    14x60 Hercules Ajax lathe
    Gorton I-22 MastrMil
    Landis 6x18 surface grinder
    20" Powermatic bandsaw
    Ancient, big drill press
    350 pound anvil and a bunch of hammers
    If I can't fix it I can make it.....unrecognizable.

  7. #7

    Default

    most the stuff i weld is aluminum heads , need lots of amps and some heads i use mix gas .

Similar Threads

  1. Another Canuck on board
    By DrunkenMoose in forum Introduce Yourself
    Replies: 1
    Last Post: 08-16-2016, 10:41 PM
  2. Missouri is on board!
    By CGCINC in forum Introduce Yourself
    Replies: 3
    Last Post: 12-10-2011, 06:36 AM
  3. New to the Board
    By TD2593 in forum Introduce Yourself
    Replies: 2
    Last Post: 08-05-2011, 12:37 PM
  4. New Owner and Member in Washington State
    By WaWelder in forum Introduce Yourself
    Replies: 2
    Last Post: 03-13-2011, 04:58 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •