    Default Mobile Home Trailer Project 3 Mean Green Contest

    Got a call today from a guy who is repossessing a double wide trailer home or mobile home. He needed the coupler welded up, and I was thinking coupler as in regular on a trailer but larger. So I broke out the Power Arc 200 and my generator and went to work. I burned 8lbs of 7018 1/8 welding rods at 129 amps. The job took about 4 hours of non-stop welding, this is the hardest I have pushed my Power Arc 200, never bumped the duty cycle, and never missed a beat!

    This is the view from under the house.


    This is the first pass from the under side of this coupler or A frame. I put at least 3 passes on every weld. This frame was not fitted very well, so there were several passes on most of the welds.


    One side welded on the topside.




    This is the complete frame


    This deal was provided by the guy moving the home for the bank. They were happy with how it turned out. The welder in me wanted to beef up the coupler, but there is not much to weld to underneath. Everything is pretty thin, I guess the shape of the house and that it's only designed to be transported once, and not pulled everyday.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  2. #2

    Default

    Quote Originally Posted by SeanMurphy265 View Post
    This deal was provided by the guy moving the home for the bank. They were happy with how it turned out.

    That's what counts. Now they know who they can call in the future. Could turn into a nice set of jobs if they get more to do.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

Similar Threads

  1. Project 5 Mean Green Contest, SeanMurphy265, Mobile Home Leaf Spring Mounts
    By SeanMurphy265 in forum Heavy Equipment and Commercial Projects
    Replies: 3
    Last Post: 05-23-2012, 01:26 AM
  2. Project #2 Mean Green Contest -- Insulated Smoker!
    By SeanMurphy265 in forum Other Custom Fabrications
    Replies: 12
    Last Post: 04-10-2012, 01:18 AM
  3. Replies: 4
    Last Post: 03-31-2012, 10:01 PM
  4. Project #1- Mean Green Contest --- Welder Cart
    By Bigwilly01 in forum Other Custom Fabrications
    Replies: 0
    Last Post: 03-31-2012, 03:50 AM
  5. Mean Green Contest - Project 1 - Jeep Bumper Support
    By SeanMurphy265 in forum On Road Fabrication
    Replies: 0
    Last Post: 03-19-2012, 09:10 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •