Share
Page 2 of 2 FirstFirst 12
Results 21 to 22 of 22

Thread: How you price out a welding job?

  1. #21

    Default

    Quote Originally Posted by MigPlazArc View Post
    Sounds like a good flat charge to me...although don't know if somebody that wants a bolt welded on, not sure if they would want to pay $35 lol
    Guess that depends on how badly they need a bolt welded on something.

    Even if they bring it to you, $35 is not really that bad. You have the machine, right consumables and overhead. You know the amps, have to prep it, etc.

    If you think about it.

    $20 would sound cheap, but my son does little things like that all the time if they come up and he is in the middle of welding something else.

    I think you really have to play it by ear to get started. Like anything else.

    Also, we have 5 trailers to do this weekend from a repeat customer. Treat them right and they will bring you more work too.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  2. #22

    Default

    Quote Originally Posted by CGCINC View Post
    True... . If it's a 1 minute job then I will adjust accordingly. Maybe knock off 2 bucks
    Hahahahahahah. Yeah, that that sounds about right...




    Quote Originally Posted by everlastsupport View Post
    Guess that depends on how badly they need a bolt welded on something.

    Even if they bring it to you, $35 is not really that bad. You have the machine, right consumables and overhead. You know the amps, have to prep it, etc.

    If you think about it.

    $20 would sound cheap, but my son does little things like that all the time if they come up and he is in the middle of welding something else.

    I think you really have to play it by ear to get started. Like anything else.

    Also, we have 5 trailers to do this weekend from a repeat customer. Treat them right and they will bring you more work too.
    Hahaha and yeah.
    Last edited by MigPlazArc; 04-21-2012 at 02:00 PM.
    Benjamin

    Owner of IMIG 200 and half owner of Power Plasma 50

    https://www.facebook.com/BenjaminRootPhotography

Similar Threads

  1. Argon Tank price?
    By Elantramax1 in forum General Welder Questions
    Replies: 38
    Last Post: 02-05-2015, 11:18 PM
  2. Introductory price for new Tig Torch
    By Titan winch in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 03-31-2012, 05:09 PM
  3. I would like a price quote
    By rcnut223 in forum Everlast Announcements, Contests and Promotions
    Replies: 1
    Last Post: 12-01-2010, 02:51 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •