All system well welding 1/16 in 3003 aluminum with 75 /25 helium argon mix works wonderful ! Thanks everlast! Dan Murphy
All system well welding 1/16 in 3003 aluminum with 75 /25 helium argon mix works wonderful ! Thanks everlast! Dan Murphy
You'll have to post up some pics!!
Welcome to the Everlast family!!