betokasu 6010 Arc Force settings 04-20-2012, 09:23 AM
geezer The PowerArc 200 doesn't have... 04-20-2012, 08:13 PM
undercut I'm saving up for my first... 04-28-2012, 02:52 AM
Rodsmachineshop http://www.hobartwelders.com/e... 04-28-2012, 03:02 AM
Previous Post Previous Post   Next Post Next Post
  1. Default 6010 Arc Force settings

    Hello all,

    can anybody tell me the best arc force settings for the 6010 (Fleetweld 5+, 3/32) with the Everlast PowerArc 200 ?

    Thanks in advance !

  2. #2

    Default

    Quote Originally Posted by betokasu View Post
    Hello all,

    can anybody tell me the best arc force settings for the 6010 (Fleetweld 5+, 3/32) with the Everlast PowerArc 200 ?

    Thanks in advance !
    The PowerArc 200 doesn't have arcforce settings,,,it is adaptive,,,you must mean amp settings,,,,try 50 to 60 amps for that size of rod and remember it's not a drag rod like 7014 it has a longer arc gap (dist from rod to metal) slightly greater than 1/8 inch once the arc is struck,,,,that's why they make scrap iron so you can play and practice on pieces until a fellow gets a feeling for different new rods...hope this helps you
    Some of those lies people tell about me, are true

  3. #3
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    I'm saving up for my first welder. Don't have a lot of experience - will be self-taught! I'm looking at entry-level welders so they won't have user-adjustable arc force settings. Is this feature something I should be seriously considering or will adaptive arc force be "good enough"? The jump is pretty big $-wise. Well, for me it is anyways.

  4. #4

    Default

    http://www.hobartwelders.com/elearning/ amps 40-85 DCEP: DC, Electrode Positive (reverse polarity) has the most weld penetration this mite help
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	electrode_chart.jpg 
Views:	1555 
Size:	20.5 KB 
ID:	6369  
    Last edited by Rodsmachineshop; 04-28-2012 at 03:23 AM.
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

Similar Threads

  1. 250ex Arc Force not working?
    By Monty in forum Stick Welding (SMAW)
    Replies: 2
    Last Post: 08-21-2016, 12:58 AM
  2. Arc Force Question
    By plumber in forum Stick Welding (SMAW)
    Replies: 30
    Last Post: 01-23-2013, 02:05 PM
  3. Arc Force
    By Buzz in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 01-19-2012, 05:24 AM
  4. A few questions about the ARC Force knob on my 250EX??
    By CGCINC in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 12-06-2011, 02:06 AM
  5. What is arc Force?
    By pmill607 in forum General Welding Questions
    Replies: 2
    Last Post: 08-26-2010, 01:09 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •