  1. Default AC / DC Setting is backwards?

    I have a PowerTig 185 that I've been trying to get dialed in.

    I'm trying to weld 18Ga automotive sheet metal. Not even trying to use filler rod; just running the electrode across the metal to see if I can form a puddle. I have a pretty fair amount of experience with MIG welding and understand the concepts of TIG.

    On the DC setting using orange tungstens, I always melt the electrode almost immediately. Gas is set to 15. Arc appears to be good. The welder is only set to 35 to 45. After a few seconds I notice I'm losing the arc and if I check the tungsten it has balled up under the cup.

    If I change the setting to AC, then I notice that the electrode appears to have a louder arc, but I'm able to properly puddle the metal and the tungsten doesn't turn into a ball as I'd expect it to do on the AC setting.

    This doesn't make any sense to me, but I'm wondering if anyone has an idea of what might be going on here. Is there any chance that the switch could be backwards? How would I check to find out for sure?

    Jon

  2. #2

    Default

    When you say electrode are you talking about the tungsten or the filler rod? If your talking about the tungsten you may have your polarity reversed. The tig torch should be connected to the negative terminal, and your ground clamp should be connected to the positive terminal.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  3. Default

    Quote Originally Posted by SeanMurphy265 View Post
    When you say electrode are you talking about the tungsten or the filler rod? If your talking about the tungsten you may have your polarity reversed. The tig torch should be connected to the negative terminal, and your ground clamp should be connected to the positive terminal.
    You nailed it. I'm an idiot.

    Had the ground on - and the torch on +.

    I'm going to give this another run tonight and report my results.

    Jon

  4. #4

    Default

    Should be completely different results. No need for 45 percent, and get rid of that orange/ceriated tungsten. Use red or lanthanated. Cerium won't hold the heat as well.

Similar Threads

  1. Erractic arc at low AC setting
    By Sage Hill in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 9
    Last Post: 02-14-2016, 10:59 PM
  2. What is Your Pre-Flow Setting
    By NRM in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 08-09-2012, 01:57 AM
  3. 250EX Amp Setting Changes??
    By CMB in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 08-11-2011, 03:13 AM
  4. forums backwards
    By shawn in forum Forum related Questions
    Replies: 2
    Last Post: 04-03-2011, 11:51 PM
  5. Pulse setting of PM 205
    By www in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 08-05-2010, 10:32 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •