  1. Default I got my new PM205

    Well a week or so ago I ordered a everlast PM 205. I unpacked it got a plug and started setting up. So far I have only used the plasma cutter and this thing rips I have used other brand cutters and this is by far the best one yet. I'll keep this thread updated on the welder functions as soon as I figure them out haha(I was a lincoln guy).











    these are kegs I cut the tops off of took less then 5mins to do both. AWSOME.....
    Last edited by nooch8it; 12-07-2009 at 05:24 PM.

  2. Default

    Here is my first shot at welding stainless steel. They are 1/2" fittings in the side of a keg. Let me know what I can do to improve my skills. Thanks


  3. #3

    Default

    Nooch,

    You need to get comortable and relax. It looks pretty good.

  4. #4

    Default

    The weld looks fine, as Mark said relax and take your time. If you slow down you may need to back off the heat a tad. What are you making?
    Wayne

  5. Default

    I home brew beer and I'm making a full 3 tier brew system. I have a few more to weld so I'll try slowing down and see how that works Thanks guys.

  6. #6

    Default

    If the weld is going to contact consumable product make sure to properly clean the weld with a fresh stainless steel brush and passivate the area to ensure there are no harmful contaminates. A single speck of rust could ruin a batch of good brew and make some one very ill. Here is a link that may help. In the article they mention using a citric acid solution, this works well and you can purchase it online.
    Hope this helps and good luck with the brew!
    Wayne

    http://www.mmsonline.com/articles/ho...eel-parts.aspx

Similar Threads

  1. 3/8th Aluminum with my PM205
    By www in forum TIG Welding (GTAW/GTAW-P)
    Replies: 30
    Last Post: 03-29-2011, 05:37 AM
  2. 30 amp breaker for PM205
    By www in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 12
    Last Post: 04-27-2010, 05:57 PM
  3. Just set up my new PM205
    By xen808 in forum Customer Testimonials
    Replies: 1
    Last Post: 03-17-2010, 08:55 PM
  4. having some problems with my PM205
    By racinjason44 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 11
    Last Post: 03-15-2010, 11:44 PM
  5. PM205 L10-50R Plug Wiring
    By jas329 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 5
    Last Post: 01-13-2010, 06:20 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •