    I finally got home and had a chance to play with my 200DX. I had to wire in a plug, and had a few issues with that. Once I got that squared away, plugged in my welder. Nothing.

    I called tech support and apparently I wired the plug wrong on the welder. Re-wired the plug, turned it on, and I was in business.

    I bought a shield, and gloves. I had some 6011 1/8 rods I had from work. Hooked everything up, and started burning rods. I'll have to say, this thing welds sweet. I can't wait to start to TIG on in in the next couple of days. I have to get a bottle of gas, then I'll be in business.

    Also, I don't think the torch is too big for me. So I am good to go!

    So far, very impressed. I heard technical support sucked. That's a lie. All my stuff will be green from now on.

    Thanks again Everlast. You have my vote.
    Purple Fabricator 211i

  2. #2

    Default

    Ahhh...yes, the plug issue. I am working on a video that will deal with how to wire all our units.

  3. #3

    Default

    I can make one in the morning.
    Purple Fabricator 211i

  4. #4

    Default

    When you start using the TIG make sure you post an update ... The 200DX is the unit I'm planning on buying as soon as I qualify for the 25% discount ... wish I didn't have to wait. As far as wiring goes ... Just remember ... "green is ground, the world around" Sorry I couldn't help myself LOL
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

  5. #5

  6. #6

    Default

    can you change your welders color to purple since i like purple lol
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  7. #7

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    can you change your welders color to purple since i like purple lol
    We had a guy years ago that would air brush and eagle of anything you like. Did not get over big. My son has a Ford blue wants to paint one in, but I will not let him. I do have an old CK 140 MIG/TIG (monster) I can let him paint. Trying to sell it. New paint might do it.

    Glad 225 is enjoying the new welder. Post up some picture if you get time.

    Scary, I like purple myself (but on a old hot rod).
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  8. #8

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    can you change your welders color to purple since i like purple lol
    I am a LSU fan and everything I have is purple and gold.

    I like the green. But the green forum is too much. Since I own vBulletin forums, y'all outta let make a new style. I'll email y'all the XML file, and tell me what yall think.
    Purple Fabricator 211i

  9. #9

    Default

    Quote Originally Posted by 225 View Post
    I am a LSU fan and everything I have is purple and gold.

    I like the green. But the green forum is too much. Since I own vBulletin forums, y'all outta let make a new style. I'll email y'all the XML file, and tell me what yall think.
    I thought he was talk about the welder color?

    Sure send it over and instructions. Can we add it as an extra theme? Then people can pick. Believe it or not, people like this as well and it has grown on me as well. You know you are on the Everlast forum.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  10. #10
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by everlastsupport View Post
    You know you are on the Everlast forum.
    You're not kidding. Can't miss it - even from across the house!
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  11. #11
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    Quote Originally Posted by 225 View Post
    I like the green. But the green forum is too much. Since I own vBulletin forums, y'all outta let make a new style. I'll email y'all the XML file, and tell me what yall think.
    You should have seen the color scheme about a year and a half ago. (It's much improved now.)

    http://www.everlastgenerators.com/fo...e-eyes-that-me
    '13 Everlast 255EXT
    '07 Everlast Super200P

  12. #12

    Default

    I like the green! I am a member of MANY web forums and this is by far the easiest on the eyes. I'm interested in how you like the 200dx as I am also thinking of using my 25% off discount on that unit (maybe). But I guess that depends on if I actually get to 100 or not
    Last edited by lucky13; 05-14-2012 at 05:47 AM.
    Newbie welder with just a Campbell Flux Core 80 watt "hot glue" gun, for now........

  13. #13

    Default

    I am putting stick on purple flames on all my everlast welders lolClick image for larger version. 

Name:	fyVMtP8A.jpg 
Views:	365 
Size:	5.6 KB 
ID:	6605
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  14. #14

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    I am putting stick on purple flames on all my everlast welders lolClick image for larger version. 

Name:	fyVMtP8A.jpg 
Views:	365 
Size:	5.6 KB 
ID:	6605
    I have cut them here too. Just no purple vinyl here.. I probably have other wild colors.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  15. #15
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    can you change your welders color to purple since i like purple lol
    Can't do it, Rod. Can you imagine the backlash if these forums went all purple? LOL
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

Similar Threads

  1. PowerTig 200dx question
    By AnimalMother in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 02-25-2016, 01:44 AM
  2. PowerTIG 200DX
    By Sparky_Mark in forum Pre-sales, Sales and Shipping questions
    Replies: 4
    Last Post: 10-18-2015, 04:09 AM
  3. powertig 200dx problem
    By babowtie in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 4
    Last Post: 02-01-2015, 04:30 PM
  4. Buy the Powertig 200dx or save for The Dynasty 200dx
    By AfroPaul in forum TIG Welding (GTAW/GTAW-P)
    Replies: 40
    Last Post: 05-13-2013, 07:18 PM
  5. PowerTig 200DX Cover
    By earla in forum Other Custom Fabrications
    Replies: 2
    Last Post: 09-01-2011, 12:23 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •