I am working on my first project using 304 Stainless tubing. The tubing that I am working with varies in diameter from 1.75" to 3.5". All of the tubing is around .065" thick. Most of the joints are butt welds and I have been trying real hard to keep the fit up tight. The problem I am having is the welds end up with little to no color. They look grey and dull. During my many hours of practice, the only time I seem to be able to get a nice looking weld is when fusion welding the tubing. As soon as I add filler the weld turns grey.
200DX welder
#8 Gas Lens
Tried 30-70 amps with the sweet spot around 50 it seems
Also tried with pulse and without.
Gas flow around 7-10 L
Tried with back purge and without back purge with no noticeable change
Tried 1/16 tungsten and 3/32 tungsten. 3/32 seems to have a more stable arc
Tried 2% Ceriated, 2% Thoriated and bought but haven't tried Lanthaniated Tungsten.
Have been using .045" 316L filler rod
I'm just getting frustrated with the lack of improvement on the welds. I have had no problem with steel or aluminum, but this Stainless is kicking my butt. I really would like to be able to get a nice looking strong weld. I forgot to grab my camera from home. I will post up some examples of the welds tonight.
Thanks for the help,
Chris


 
					
					 
							
						 Stainless Tubing Help
 Stainless Tubing Help
		 
				
				
				
					 Reply With Quote
  Reply With Quote

 Originally Posted by Injected65
 Originally Posted by Injected65
					
 
				