    Hi, I am interested in buying A PP50 for a primary cnc torch But i will also be cutting some 3/8 ar500 for steel targets on a water table, On some targets i will need to pierce some mounting holes, will the PP50 be able to do this? and if know one knows I would like to send a piece to someone who owns the PP50 and give it a try before i purchase this model of plasma cutter.
    Thanks Jim

  2. #2

    Default

    it cut 3/8 with no problem good for a plasma cnc table but would recommend getting a new arc divider board if going to use a thc control that torch height control . you need that if cutting a not flat piece of metal i have some stuff 3/8 and thicker stuff at my shop i will cut with 50 and post some pics i have cut 1/2 with a nice clean cut . see your in arizona so am i i live in Parker AZ
    Last edited by Rodsmachineshop; 05-14-2012 at 07:00 AM.
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  3. #3

    Default

    Cutting and pierceing are two different things,,the rule of thumb for pierce is,,,20 amps for every 1/8 inch,,,not an exact rule but a good one,,I have a PP50 and a PP80,,,both good machines,,,the PP50 will do your 3/8 ar500 material.
    Some of those lies people tell about me, are true

Similar Threads

  1. Power Plasma 50 plasma cutter....
    By CGCINC in forum Customer Testimonials
    Replies: 4
    Last Post: 07-20-2012, 01:58 PM
  2. Power Plasma 50 help.
    By dean_af in forum Everlast Plasma Cutters (PAC)
    Replies: 11
    Last Post: 10-04-2011, 04:46 PM
  3. power plasma 50
    By cmd in forum Customer Testimonials
    Replies: 0
    Last Post: 09-15-2010, 02:52 AM
  4. My Power Plasma 50
    By jtybt in forum Everlast Plasma Cutters (PAC)
    Replies: 27
    Last Post: 04-28-2010, 09:08 PM
  5. power plasma 50
    By brucewelding in forum Everlast Plasma Cutters (PAC)
    Replies: 1
    Last Post: 03-06-2010, 01:04 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •