Anyone have any tips or tricks to welding nuts to pipe? I'm actually welding 1/4" nuts to 1/2" coupling nuts.
Last time I put the bolt through the nut tacked and partially welded the nut and the bolt started sticking as the weld was cooling. Barely got it out and had to tap the nut to get another bolt in.