  1. Default Foot Pedal and Arc Start

    Most of the stuff I weld is SS at about 90-100A or so. Last weekend I was welding some nuts and the amperage was set at 75A. I noticed when I was using the foot pedal that the arc would start a little later than usual as I depressed the pedal. Is this because the amps were lower than usual or is the pot wearing? The arc would start just a fraction of a second later than usual but I could still tell the difference. Anyone else notice this?
    PowerPro 205
    9" South Bend Lathe
    Enco Mill/Drill
    Evolution Rage 2

  2. #2

    Default

    You have upslope turned up or more preflow?

  3. #3

    Default

    It seems like if I have "start amps" turned down too low it won't start or will be a little delayed... Just a thought
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  4. Default

    Mark I don't think so but I will check. CGC I have start amps turned down to the minimum, but I will check that also.
    PowerPro 205
    9" South Bend Lathe
    Enco Mill/Drill
    Evolution Rage 2

Similar Threads

  1. Anyone doing scratch start TIG with a Power Arc ? (Adding a pedal ?)
    By someguy in forum TIG Welding (GTAW/GTAW-P)
    Replies: 12
    Last Post: 08-02-2012, 01:22 AM
  2. new foot pedal
    By hesstx in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 12-16-2011, 05:26 PM
  3. Bad foot pedal?
    By sth212 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 08-21-2011, 08:50 PM
  4. Erratic start with foot pedal
    By jtybt in forum TIG Welding (GTAW/GTAW-P)
    Replies: 27
    Last Post: 08-03-2011, 05:40 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •