I probably brag more about the 250EX than most, Our first 250Ex was bought used and had been tuned up by a local shop to weld at specs, It had different resistance pots on the pulser and ac balance. It will pulse at .1pps and adjust all the way down to no cleaning action if needed, With red tungsten I can weld at 250 amps on AC and keep a sharp tungsten ( super sharp), no dingle berries and no tungsten splitting. I can go for days without sharpening the tungsten on AC.
When I got the new 250EX, it would only pulse at 1pps and would only adjust to about 60% electrode negative with about 1/4 inch cleaning action minimum, and would not hold a sharp point. After talking to Oleg, he authorized these mods for the new 250EX and now it welds as good as the first. Hopefully these mods will added to the newer models.
After having a super stable arc cone way down on the tip of the tungsten, it would be hard to go back to a machine that has a dancing arc.
Posting Permissions
- You may not post new threads
- You may not post replies
- You may not post attachments
- You may not edit your posts
-
Forum Rules