Quote Originally Posted by EmptyNester View Post
Unfortunately, its a little leaky as pools go. I went through one round of patching holes but still have some left.

I probably shouldn't have painted it until after I tested. Now I'm not sure how I'll get the paint out of the corner that needs "patched".
This is true. You also don't know if the paint is sealing other very small leaks. When I used to build oil pans, I found that testing for leaks with solvent or mineral spirits is better than water. Less surface tension and it seems to find everything.
I'm sure a little heat and a wire brush will burn the paint out of your corners enough to re-weld them. MIG and stick can be pretty forgiving about bits of paint, at least. Of course just coating with a sealer is the easy way out.