Thread: Melted 250 ex torch

  1. Default Melted 250 ex torch

    I was told I could use torch without water cooler as long as I did not go over 200 so I kept it at 130 and it still melted wtf I guess its time for the weld craft 300 wasn't a big fan of the torch but I only used it a few times but the welder was pretty nice welded just as well as a dynasty 200 I do a lot of field work and dont have time to lug the cooler around with me

  2. #2

    Default

    nope did the same thing . have to run water cooling . i got a air cooled torch when i weld mobile and use the water cooled at shop
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  3. #3

    Default

    Quote Originally Posted by Redhead View Post
    I was told I could use torch without water cooler as long as I did not go over 200 so I kept it at 130 and it still melted wtf I guess its time for the weld craft 300 wasn't a big fan of the torch but I only used it a few times but the welder was pretty nice welded just as well as a dynasty 200 I do a lot of field work and dont have time to lug the cooler around with me
    Redhead

    when did you buy the unit ?

    let me see what i can do for you ?
    Oleg Gladshteyn
    Phone: 650 588 8082 / 877 755 WELD
    Cell: 415 613 6664 ONLY IF YOU REALLY NEED IT
    Email: oleg@everlastwelders.com
    Website www.everlastgenerators.com

    www.linkedin.com/pub/oleg-gladshteyn/48/b08/875

  4. #4

    Default

    Quote Originally Posted by Redhead View Post
    I was told I could use torch without water cooler as long as I did not go over 200 so I kept it at 130 and it still melted wtf I guess its time for the weld craft 300 wasn't a big fan of the torch but I only used it a few times but the welder was pretty nice welded just as well as a dynasty 200 I do a lot of field work and dont have time to lug the cooler around with me
    I think the way it should have been stated. You can use a non water cooled torch under 200 but over 200 you need a water cooled torch. I don't think you can use a water cooled torch, without water, at all.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  5. #5

    Default

    If you stay close to a water hose, no need for a cooler. The water hose can be bushed down to work on the torch, and all you need is a nice flower bed that needs a little free water on it.

  6. #6

    Default

    I've used my water cooled torch up to around 120-130amps. Not continuous but for small welds and I'm too lazy to lean over and turn on the cooler...
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  7. #7
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by CGCINC View Post
    I've used my water cooled torch up to around 120-130amps. Not continuous but for small welds and I'm too lazy to lean over and turn on the cooler...
    But at least your power cable was filled with water. Without that, they only last seconds. The power cable in a typical water cooled setup is only about 10 gauge wire, it really depends on the fluid to stay in one piece. Compare that with the size of your ground cable...
    Long arc, short arc, heliarc and in-the-dark!

  8. Default Tig torch

    Quote Originally Posted by Oleg View Post
    Redhead

    when did you buy the unit ?

    let me see what i can do for you ?
    Bought it a few months ago but just received it a few weeks ago because of backorder I like the machine but not happy with info I had received about using torch I hear you will be in my area for farm days could I talk with someone there I happen to live in the same town

  9. #9

    Default

    Quote Originally Posted by Rambozo View Post
    But at least your power cable was filled with water. Without that, they only last seconds. The power cable in a typical water cooled setup is only about 10 gauge wire, it really depends on the fluid to stay in one piece. Compare that with the size of your ground cable...
    Ahhhhh... the water in the line Would help!
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  10. Default

    Quote Originally Posted by Redhead View Post
    I was told I could use torch without water cooler as long as I did not go over 200 so I kept it at 130 and it still melted wtf I guess its time for the weld craft 300 wasn't a big fan of the torch but I only used it a few times but the welder was pretty nice welded just as well as a dynasty 200 I do a lot of field work and dont have time to lug the cooler around with me
    what torch were you using on the dynasty?

  11. Default

    I think it was a ck 17 air cooled

  12. Default

    I melted down my WP17 as well. The hose that goes over the power conductor is nylonish and it doesn't take much heat. Its not rubber like the jacket on a welder cable.

    All I need is new hose and a seath and mine will be as good as new. I've got it rewired as an air cooled torch using a piece of welder cable for now.

  13. #13

    Default

    A 17 is limited to 150 amps DC and somewhere around 125 AC. If you go over that, you are asking for troubles. Are you referring to the WP 18?

  14. #14
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by someguy View Post
    I melted down my WP17 as well. The hose that goes over the power conductor is nylonish and it doesn't take much heat. Its not rubber like the jacket on a welder cable.

    All I need is new hose and a seath and mine will be as good as new. I've got it rewired as an air cooled torch using a piece of welder cable for now.
    WP9, WP17 are air cooled while WP20, WP18 are the water cooled versions that share the same hardware. Be careful using a water cooled torch with a plain cable. Not only are the power cables cooled by the water, the torch is too. You can overheat the torch head and ruin it, running it without water. If you want air cooled, get an air cooled torch and cables.
    Long arc, short arc, heliarc and in-the-dark!

  15. Default

    Just ordered a weld craft 300 air cooled torch that should fix my problem thanx for all the advice live and learn I guess.

  16. #16

    Default

    Quote Originally Posted by CGCINC View Post
    I've used my water cooled torch up to around 120-130amps. Not continuous but for small welds and I'm too lazy to lean over and turn on the cooler...
    I am thinking about wiring my cooler to the welder side of the switch/breaker so the cooler automatically comes on when welder is on, assuming the cooler switch is on.
    Millermatic 251 with 30A
    Synchrowave 180
    Hobart 100 MIG
    lathe & RF45
    Power TIG 250EX
    Spectrum 625 X-TREME
    Spray Zone.net-Side draft spray booth

  17. #17

    Default

    that's what i did i rewired my 250ex so when welders turned on the cooler comes on also
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

Similar Threads

  1. Floating head Machine Torch holder w/ S45 Machine Torch - 2 for sale.
    By countryguy in forum Everlast Plasma Cutters (PAC)
    Replies: 2
    Last Post: 12-19-2016, 10:52 PM
  2. Melted my torch!
    By BillC in forum General Welder Questions
    Replies: 8
    Last Post: 06-06-2016, 04:37 PM
  3. Change tig torch to a smaller water cooled torch
    By wheelrdealer in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 4
    Last Post: 09-18-2012, 05:07 PM
  4. Model 26 Torch & General Torch Questions...
    By Ray C in forum TIG Welding (GTAW/GTAW-P)
    Replies: 14
    Last Post: 08-26-2012, 04:47 PM
  5. purple torch or S45 torch the best
    By trickbiker in forum Everlast Plasma Cutters (PAC)
    Replies: 3
    Last Post: 12-06-2011, 03:58 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •