    Hello all,
    I have a PP50. It has worked flawlessly until today. The last use was a week or so ago. It worked fine. I finished the cuts, let the fan run for a few and then shut the machine down. Today I went out to make some cuts and.....Problem!
    Turned machine on, All is well.
    Checked air pressure, all is well.
    Grounded the metal, pulled the trigger, I got air flow, but no pilot arc or cutting.
    Checked the swirl ring, all is well.
    Replaced the electrode, same thing.
    replaced the tip, same thing.
    Adjusted post flow, switched from constant to timed and back several times, no change.
    Switched from 2T to 4T and back, no change.

    Is there an adjustment for the pilot arc? like a contact gap or something?
    My machine sits on a dedicated cart with a dedicated air line, hard wired by an electrician.
    Any help is appreciated.
    Josh
    Last edited by WaWelder; 08-01-2012 at 03:56 AM. Reason: added swirl ring comment
    When opportunity knocks, most do not recognize it, because it shows up wearing overalls and looking like work!!
    Joshua,Tacoma,Wa
    24'x48'shop-6/2010
    Hobart Handler125w/125cf 75/25-1998-Welds perfect
    Power tig250EX-w/300cf argon-2/2011-had 4053 problem, fxed and good as new
    Power Cool W300-4/2011-works great after making hoses
    Power Plasma 50-4/2011-in for repair
    Shop air

Similar Threads

  1. New diy cnc machine pp50 with thc
    By waynagen in forum Everlast Plasma Cutters (PAC)
    Replies: 17
    Last Post: 01-13-2014, 02:14 PM
  2. PP50 arrived with familiar problem
    By keweenawbee in forum Everlast Plasma Cutters (PAC)
    Replies: 10
    Last Post: 11-14-2012, 11:03 PM
  3. PP50 arc issues
    By millermatic in forum Everlast Plasma Cutters (PAC)
    Replies: 7
    Last Post: 09-29-2012, 11:14 PM
  4. PP50 cup
    By jtybt in forum Everlast Plasma Cutters (PAC)
    Replies: 8
    Last Post: 04-21-2010, 05:54 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •