Ok. The problem we see with hard starting can be attributed to the helium. Really don't like to see that much helium used, if at all because it gives the arc fits at start, and the helium and argon segregate and provide poor coverage at times. But that does not explain no power. As I said, we'll do something as quick as possible. Oleg and Ray are aware. Going to get an answer tomorrow, since it was late today.