Hi... I'm wondering if folks could tell me about the differences in hood brands or models. I tried searching the forum and didn't come up with too much.
Right now, I have a Harbor Freight auto-darkening hood (cost about 49 or 59 bucks) and it seems OK but I have no comparison. I use "cheater" magnifier lenses that are miller brand but they don't quite fit but stay on fine with a little piece of duct tape. For TIG and stick, I usually set the darkness between 9 and 10 and it suits me OK. After 3 years of a lot of use, its holding up well and I've had to make and install a new sweat band. Since I just got setup to do TIG, my welding time is about to double or triple and since I only have 1 hood, I'm thinking about getting a backup.
Anyhow, just wondering if folks could tell me what makes one hood better than another. This could be one of those situation where almost everybody has settled on the same brand after some trial and error -and I'm trying to save myself from that "error" part...
BTW: Maybe I'm paranoid but every day when I start using the hood, I start-out with a test with the flint starter to make sure it's working. It would really suck if you struck an arc and that thing didn't go dark.
Thanks
Ray




Reply With Quote