  1. #1

    Default 250 ex

    I was welding with my 250 ex today on an oil pan and was having a hard time keeping a smooth and consistant arc had to kind of scratch start it sometimes and when it was welding it would kind of go off and on while i was welding but the arc would stay on just kind of jumped around .Does this sound like a point gap issue or something else?

  2. #2

    Default

    what do you have your gas set at . i set mine 250 ex at 9 to 10 lpm if not enough argon arc start will be erratic but also could be point not set rite also , aluminum pan or steel pan
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  3. #3

    Default

    steel pan,and my gas was set at around 7 ..cant remember what points are supposed to be set at.

  4. #4
    Join Date
    Oct 2010
    Location
    Nova Scotia, Canada
    Posts
    143

    Default

    Did you try welding something else? Sounds sort of like contaminated material to me.
    HF is shut off after starting, so it's not a point gap problem.

  5. #5

    Default

    Quote Originally Posted by Paul Moir View Post
    Did you try welding something else? Sounds sort of like contaminated material to me.
    HF is shut off after starting, so it's not a point gap problem.
    DITTO!

    Double check all connections are tight and confirm machine settings and try on some fresh ground steel.
    Millermatic 251 with 30A
    Synchrowave 180
    Hobart 100 MIG
    lathe & RF45
    Power TIG 250EX
    Spectrum 625 X-TREME
    Spray Zone.net-Side draft spray booth

  6. #6

    Default

    could be contaminated material as it is an oil pan but the material i was welding on the oil pan was new material ,cut the side out of the front of the oil pan and had to put a half moon shaped piece back in to make room for a starter ,so i dont think contaminated material was all of the problem and i did have to keep scratch starting the tungsten to start the arc.

  7. #7

    Default

    have you tried using a new tungsten electrode and everything is tight on the torch
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  8. #8

    Default

    did not try using a new tungsten but did have to re-sharpen and everything is tight on my torch,i use both thoriated and lanthanated tungsten.