bad tank of gas . i have got 2 or 3 bottles of bad gas argon and co2 and argon mix . I asked Jessie from A&B gas he tells me its the guys being lazy when checking and filling tank he says the killer is having air or oxygen in the tank before filling .he say happens when welder run a tank empty and after removing welding gauges leaves tank valve open condensation forms and air gets in tank , the fill guy when see a tank with a valve open or empty totally is suppose to purge tank with argon and evac tank before refilling , he just fired one of his guys because it cost money for bad gas fills and dosnt look good for his business. think i will make a dryer for my argon hose lol