    Upon pressing the trigger the arc will start then when a load is put on the arc it goes out then re-arcs. It cuts really well I have no other issues other than the pressure regulator fluctuates when the trigger is pressed is that suppose to happen? Thanks for any help.
    CMILL
    Millermatic-211
    Thermal Arc 300 GTSW
    Everlast PP50

  2. #2

    Default

    It sounds like you have an air pressure problem. Too much or too little at the wrong time. What size air compressor are you using?

  3. Default

    It runs 8scfm at 90 psi, that makes sense because I can't run it at the same time due to breaker issues. It's a 25 gal 6 hp craftsman professional
    CMILL
    Millermatic-211
    Thermal Arc 300 GTSW
    Everlast PP50

  4. #4

    Default

    What's your "Operating" air pressure when it is cutting? What amps are you running at?
    How much drop in air pressure are you getting when you press the trigger? If it's more than 5-7 psi, the unit may have a kinked hose going to the air gauge.

  5. Default

    Thanks guys ill make sure the compressor can be plugged in at the same time as the cutter, so i can get ample air pressure.
    CMILL
    Millermatic-211
    Thermal Arc 300 GTSW
    Everlast PP50

Similar Threads

  1. pp50 problems
    By fitter in forum Everlast Plasma Cutters (PAC)
    Replies: 1
    Last Post: 07-17-2014, 03:06 PM
  2. Mystery question of the day - foot pedal for PP50 & euro connect?
    By sticks in forum Everlast Plasma Cutters (PAC)
    Replies: 5
    Last Post: 03-12-2013, 10:44 AM
  3. 185 Voltages (also PP50 question on Voltages)
    By sportbike in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 10-15-2012, 12:38 PM
  4. Having trouble with PP50
    By jtybt in forum Everlast Plasma Cutters (PAC)
    Replies: 11
    Last Post: 06-16-2011, 08:04 PM
  5. PP50 cup
    By jtybt in forum Everlast Plasma Cutters (PAC)
    Replies: 8
    Last Post: 04-21-2010, 05:54 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •