Share
Page 2 of 2 FirstFirst 12
Results 21 to 25 of 25

Thread: 250 LX Tig breakdown #1 Need help Techs !

  1. Default

    Quote Originally Posted by Vinhtec View Post
    Performance Mark, Have you guys received my machine yet? I think I might have forgotten to put my serial number on there now that I think about it. I hope you don't loose my little green giant!
    Any good news guys ?

  2. #22

    Default

    Quote Originally Posted by Vinhtec View Post
    Performance Mark, Have you guys received my machine yet? I think I might have forgotten to put my serial number on there now that I think about it. I hope you don't loose my little green giant!

    I can't look up a forum handle. Please pm me your information.

  3. #23

    Default

    Mark,

    I PMd his email. But there is nothing else on the forum like First and Last name.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  4. Default

    Hey Everlast Tech Support I been waiting 8 weeks just about for my machine and no word. Anything new? and explanation?

  5. #25

    Default

    Quote Originally Posted by Vinhtec View Post
    Hey Everlast Tech Support I been waiting 8 weeks just about for my machine and no word. Anything new? and explanation?
    You will need to call to find out the status, ext 202 or 207. 877-755-9353
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. 250 EX 5th breakdown
    By notawelder in forum Technical Bulletins and Tips
    Replies: 19
    Last Post: 10-21-2011, 03:34 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •