    Default First TIG welds

    Finally got my TIG class going- We are learning to do welds first in mild steel, then we progress to stainless Steel, And finally aluminum with 4 basic plate designs- Corner Joint, Lap weld,Butt weld, and T joint-

    My first one is merely fused with no filler-16Ga Mild steel Lincoln Precision TIG 225- set current to 90 but only use around 1/2 pedal: Click image for larger version. 

Name:	P1020209.jpg 
Views:	1248 
Size:	140.5 KB 
ID:	8025And a shot of the backside.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	P1020203.jpg 
Views:	546 
Size:	131.2 KB 
ID:	8022   Click image for larger version. 

Name:	P1020206.jpg 
Views:	495 
Size:	126.1 KB 
ID:	8023  
    Everlast PowerTig 200DX (Ordered-Waiting to arrive!)
    Everlast Supercut 50P


    Fortune Favors the bold.

  2. #2

    Default

    Here are a couple of my "Lap Joint" attempts-16ga Mild steel, 1/16" ER70S-2 filler rod, 90 amps with about 1/2 pedal argon on about 5-10 seconds post flow. What do you guys think?Click image for larger version. 

Name:	P1020204.jpg 
Views:	636 
Size:	138.8 KB 
ID:	8026Click image for larger version. 

Name:	P1020205.jpg 
Views:	540 
Size:	133.6 KB 
ID:	8027
    Everlast PowerTig 200DX (Ordered-Waiting to arrive!)
    Everlast Supercut 50P


    Fortune Favors the bold.

  3. #3
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,662

    Default

    Looks like a little undercutting on the right, but hard to tell from the pics, the flash washes a lot of detail out. Maybe try to concentrate a little more of the heat into the bottom piece. The edge piece needs a lot less than the other piece. Overall looks pretty good. Do they have you cut them up to see the cross section afterwards?
    Long arc, short arc, heliarc and in-the-dark!

  4. #4

    Default

    Quote Originally Posted by Rambozo View Post
    Looks like a little undercutting on the right, but hard to tell from the pics, the flash washes a lot of detail out. Maybe try to concentrate a little more of the heat into the bottom piece. The edge piece needs a lot less than the other piece. Overall looks pretty good. Do they have you cut them up to see the cross section afterwards?
    I am working no my technique and its not easy! keeping the torch at the right angle/speed/heat/height and all the while dipping the filler in the puddle without contaminating the tungsten! I love it! They do not cut them up to look for penatration but I am getting just a hint of a HAZ and where it looks like it almost ready to come through
    on the back side
    Everlast PowerTig 200DX (Ordered-Waiting to arrive!)
    Everlast Supercut 50P


    Fortune Favors the bold.

  5. #5

    Default

    HAZ isn't visible to the naked eye. Color change doesn't necessarily indicate the length or extent of the HAZ. The HAZ is found in the microstructure of the metal, and changes the microcystalline formations of the metal.

  6. #6

    Default

    I think it looks pretty good for your first shot. Where are you taking your classes? Local community college?
    Miller 210 MIG
    Eagle 3-Cylinder Compressor
    Air Tools
    Body Tools, Shrinker, Stretcher
    Bead Blast Cabinet
    Homebuilt Car Rotisserie

    1971 Dodge Challenger, Pro-Touring, 6.1 Hemi, Fikse Wheels, 335/275 Tires (in progress)

Similar Threads

  1. My first welds with my PA 160 STH
    By ironmanjay in forum Stick Welding (SMAW)
    Replies: 9
    Last Post: 07-25-2013, 03:23 PM
  2. A few of my first welds with the I-MIG 200.....
    By CGCINC in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 26
    Last Post: 04-23-2012, 03:46 PM
  3. My Welds
    By Oxide00 in forum Other Custom Fabrications
    Replies: 35
    Last Post: 11-09-2011, 11:23 AM
  4. how are my welds
    By dgarnier in forum TIG Welding (GTAW/GTAW-P)
    Replies: 26
    Last Post: 05-20-2011, 01:46 AM
  5. First welds
    By Ram48 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 04-07-2011, 06:04 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •