I have a PP60C that is ~5 months old, overall I have been impressed with it, but I am having problems getting good results with it on 1/4" and thicker steel. The PP60C is supposedly rated to cut over 1" thick, all I can say is I don't see how it would be possible.

I can only cut 1/4" steel at about 25ipm at about 40-45 amps to get a decent cut. This is with automatic torch height control functioning. I was cutting some 3/8" steel today and it cut fine at 20ipm if I ran it at 50-55 amps. I am perfectly fine with that, except that after about 5 minutes of cutting it stopped cutting, then started again, then stopped, etc. I can only assume this means it was running too hot and shut down for a second or two.

As many of you CNC guys might know, that causes BIG problems when something doesn't cut right the first time, ATHC won't work properly the 2nd time around, and running it without ATHC on metal that is nowhere close to flat all the way across is tough.

What amperage/speed should I be cutting at? I tried dropping the amperage down to 45 (and 15ipm) but it will barely pierce the 3/8", and even then it cuts out after cutting for a bit.

The hypertherm settings suggest 45amps at 32ipm for 3/8" steel, the PP60C (at least mine) wouldn't come close to doing that, it wouldn't cut cleanly at 45amps at 20ipm.