Columbo Aluminum welding requirements 10-19-2012, 08:40 PM
Rambozo A lot of practice and a... 10-19-2012, 08:55 PM
Columbo Yes, I had heard that Mig or... 10-19-2012, 11:40 PM
Rambozo It depends on the thickness... 10-20-2012, 12:31 AM
Columbo WOW! The reason I was asking... 10-20-2012, 04:35 AM
Shield Arc I did this Tig weld years... 10-26-2012, 10:52 AM
performance Ok, ignore the man behind the... 10-26-2012, 12:24 PM
Shield Arc Skill?! I gotta disagree... 10-26-2012, 04:14 PM
Shield Arc blacksmith there are a lot of... 10-26-2012, 08:07 PM
SeanMurphy265 By the way the older... 10-29-2012, 12:04 PM
fdcmiami that setup is serious... 10-29-2012, 03:14 PM
Previous Post Previous Post   Next Post Next Post
  1. #1
    Join Date
    Sep 2012
    Location
    Totonto, Ontario
    Posts
    27

    Default Aluminum welding requirements

    Is there any special requirements to weld aluminum with the PA200 other than using aluminum electrodes?

    Thanks.

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,662

    Default

    Quote Originally Posted by Columbo View Post
    Is there any special requirements to weld aluminum with the PA200 other than using aluminum electrodes?
    A lot of practice and a little luck. SMAW aluminum is very tricky, and the electrodes are kinda pricey. I've tried it more than once and have never been happy with the results. MIG or TIG is the prefered process for aluminum.
    Long arc, short arc, heliarc and in-the-dark!

  3. #3
    Join Date
    Sep 2012
    Location
    Totonto, Ontario
    Posts
    27

    Default

    Quote Originally Posted by Rambozo View Post
    A lot of practice and a little luck. SMAW aluminum is very tricky, and the electrodes are kinda pricey. I've tried it more than once and have never been happy with the results. MIG or TIG is the prefered process for aluminum.
    Yes, I had heard that Mig or TIG was most commonly used for aluminum but I had heard that it could also be done with stick but takes a bit of practice. I had also heard that it required a special spool for aluminum wire feed.

  4. #4
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,662

    Default

    Quote Originally Posted by Columbo View Post
    Yes, I had heard that Mig or TIG was most commonly used for aluminum but I had heard that it could also be done with stick but takes a bit of practice. I had also heard that it required a special spool for aluminum wire feed.
    It depends on the thickness of the wire and the particular machine. A spool gun is typically a more trouble free MIG solution. There are also push-pull systems where in addition to the push drive rollers in the unit, there are pull drive rollers in the gun. The big problem is that aluminum wire is soft, so it can bind up easier, and the drive rollers can't grip it as well as steel.

    For SMAW you can use E4043 electrodes, but be prepared for a little sticker shock. Standard E7018 rods are around $2.90 a pound while E4043 from the same source is $33.24 a pound.
    Long arc, short arc, heliarc and in-the-dark!

  5. #5
    Join Date
    Sep 2012
    Location
    Totonto, Ontario
    Posts
    27

    Default

    Quote Originally Posted by Rambozo View Post
    It depends on the thickness of the wire and the particular machine. A spool gun is typically a more trouble free MIG solution. There are also push-pull systems where in addition to the push drive rollers in the unit, there are pull drive rollers in the gun. The big problem is that aluminum wire is soft, so it can bind up easier, and the drive rollers can't grip it as well as steel.

    For SMAW you can use E4043 electrodes, but be prepared for a little sticker shock. Standard E7018 rods are around $2.90 a pound while E4043 from the same source is $33.24 a pound.

    WOW! The reason I was asking about the aluminum weld is that I am an amateur radio operator, (HAM), and I like making antennas which, of course, are made from aluminum tubing and square aluminum booms. I can buy a 7 foot x 2 inch square aluminum boom for that price so what makes these rods so expensive?

  6. #6
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by Columbo View Post
    WOW! The reason I was asking about the aluminum weld is that I am an amateur radio operator, (HAM), and I like making antennas which, of course, are made from aluminum tubing and square aluminum booms. I can buy a 7 foot x 2 inch square aluminum boom for that price so what makes these rods so expensive?
    Unfortunately, probably because of the low demand and maybe because of the exotic flux composition on the aluminum. People doing a lot of aluminum will usually opt for MIG or AC TIG so these rods aren't in high demand. SMAW aluminum (from what I've read) doesn't always result in very good welds either. With a TIG setup on your PA200, you could weld with a helium shielding gas but I doubt you have a helium tank just hanging around.
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  7. Default

    I did this Tig weld years ago, DCEN with 100% helium.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	100 % Helium.jpg 
Views:	535 
Size:	112.7 KB 
ID:	8322  

  8. #8

    Default

    Ok, ignore the man behind the curtain...lol.

    It takes real skill to do that...and many would question the practicality because, yes it can be done, but you need 100% He. And perfectly clean metal. He is not cheap, and Arc starts in He are terrible with most welders.

  9. Default

    Skill?! I gotta disagree there, I wouldn't make a pimple on a real Tig weldor's a$$!

    But I do agree, there is an extremely small window where the arc will start when using helium.
    The plus side is, you can almost cut your amps in half from when using AC!

  10. Default

    blacksmith there are a lot of good push pull units on the market. For years I had a Cobramatic, but the gun is not a whole lot lighter than a spool gun, and then when you add the very heavy cables too, it really gets heavy and cumbersome!

    Where people get into trouble is when trying to use a low end Mig welder, without a very short gun, with nylon liner, and proper drive rolls. When it comes to aluminum work, there is just no cheap way to do it!
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	Cobra mine.jpg 
Views:	464 
Size:	135.6 KB 
ID:	8325   Click image for larger version. 

Name:	Mig station.jpg 
Views:	427 
Size:	138.7 KB 
ID:	8326  

  11. #11

    Default

    By the way the older cobramatic setups still bring a premium on eBay. I have attempted to get a cobra wire feed setup several times $$$.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  12. Default

    Quote Originally Posted by Shield Arc View Post
    blacksmith there are a lot of good push pull units on the market. For years I had a Cobramatic, but the gun is not a whole lot lighter than a spool gun, and then when you add the very heavy cables too, it really gets heavy and cumbersome!

    Where people get into trouble is when trying to use a low end Mig welder, without a very short gun, with nylon liner, and proper drive rolls. When it comes to aluminum work, there is just no cheap way to do it!

    that setup is serious business. it almost looks like it could move under its own power.

Similar Threads

  1. aluminum welding with mig
    By rebelbah in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 2
    Last Post: 10-18-2016, 04:36 PM
  2. mig welding aluminum
    By Rodsmachineshop in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 3
    Last Post: 06-20-2012, 11:50 AM
  3. tig welding aluminum with a DC only tig
    By rab in forum General Welder Questions
    Replies: 18
    Last Post: 04-03-2012, 02:25 AM
  4. Replies: 2
    Last Post: 08-03-2011, 03:50 PM
  5. Tig welding aluminum
    By Tallguy64 in forum General Welding Questions
    Replies: 6
    Last Post: 04-10-2010, 11:02 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •